Search found 15 matches

by Gail L
Wed Jan 25, 2023 6:19 pm
Forum: Techniques and Tools
Topic: Brock Craig has passed on.
Replies: 13
Views: 296443

Re: Brock Craig has passed on.

I also saw on Facebook. Printed so many posts from him with glass help, before the internet exploded. May he rest in peace.
by Gail L
Mon Jun 22, 2015 3:07 pm
Forum: Techniques and Tools
Topic: Corelite kiln shelf questions
Replies: 4
Views: 12519

Re: Corelite kiln shelf questions

Thank you very much Brad and Dick. I'll go ahead and fire it. I appreciate all the info and you taking the time to answer ! The Warm Glass board is still the place to go when you want (accurate) info (IMO) Thank you again !!!
by Gail L
Fri Jun 19, 2015 5:57 pm
Forum: Techniques and Tools
Topic: Corelite kiln shelf questions
Replies: 4
Views: 12519

Corelite kiln shelf questions

I just received a corelite kiln shelf. Do I need to do anything special before using it ? It didn't come with instructions. I read in older threads to heat up at 200DPH. Does this mean when firing glass that I always need to take the shelf into consideration and ramp whatever project I'm working on,...
by Gail L
Mon Nov 10, 2014 9:47 pm
Forum: Techniques and Tools
Topic: Firing silver foil
Replies: 1
Views: 4685

Re: Firing silver foil

Never mind.... :mrgreen: relentless searching on my part got me the info I needed. Thanks Brad for this wonderful board that contains everything we need to know !
by Gail L
Mon Nov 10, 2014 4:27 pm
Forum: Techniques and Tools
Topic: Firing silver foil
Replies: 1
Views: 4685

Firing silver foil

I know that if the foil touches my kiln shelf, it will contaminate it. If the foil doesn't touch the shelf will I be ok ? Will the fumes from the foil have the ability to contaminate the shelf even if its not touching ? Are the fumes going to contaminate the brick in my kiln (I will vent) What temp ...
by Gail L
Sat May 04, 2013 3:43 pm
Forum: Techniques and Tools
Topic: New tutorial
Replies: 12
Views: 24184

Re: New tutorial

Going to try it with my 12 !/2" SS round from Laurie !
by Gail L
Tue Feb 05, 2013 11:02 pm
Forum: Techniques and Tools
Topic: Use for broken mold
Replies: 5
Views: 10619

Re: Use for broken mold

Thanks for the replies...its lots of pieces...
by Gail L
Sun Feb 03, 2013 11:33 pm
Forum: Techniques and Tools
Topic: Use for broken mold
Replies: 5
Views: 10619

Use for broken mold

I ordered a bowl mold from Bullseye....it was delivered by UPS...broken. The situation has been resolved (Bullseye was AWESOME) before I throw away the mold....is there any use for the broken pieces ? Different sizes of pieces. Just want to make sure I'm not throwing away broken mold pieces that cou...
by Gail L
Sun Sep 30, 2012 1:25 pm
Forum: Techniques and Tools
Topic: Covington Wet Belt Sander
Replies: 2
Views: 7417

Covington Wet Belt Sander

Just got a Covington WBS new in the box (garage sale..unbelievable !!) ....I remember reading at some point on the boards, that you could remove the back plate so that the belt has some room to move and you're not sanding on flat surface behind the belt.......not sure about the best way to use the s...
by Gail L
Wed Aug 29, 2012 11:31 am
Forum: Techniques and Tools
Topic: Problem with Slump
Replies: 16
Views: 29403

Re: Problem with Slump

Jim, I would be curious if it was 0013 Opaque white. I've used 0013 in some pattern bars, it is SO stiff that when it is fired the other glass around it flattens. It creates a little bit of a dam effect. Not sure this makes sense, but it is so stiff that its really hard to get it to move.
by Gail L
Tue Jun 26, 2012 9:26 pm
Forum: Techniques and Tools
Topic: Opaque white and specks
Replies: 0
Views: 21639

Opaque white and specks

I used BE opaque white in a pattern bar. The glass was cleaned prior to firing. There was no dirt anywhere. The slab came out of the kiln... there were black specks on and "in" the opaque white. (not many...but they are there) I cut the bar and discovered black specks contained "in&qu...
by Gail L
Mon Jun 18, 2012 4:58 pm
Forum: Techniques and Tools
Topic: Pattern Bar/Devit question
Replies: 4
Views: 9469

Re: Pattern Bar/Devit question

Thanks Brock !
Going to sandblast & FP !
by Gail L
Mon Jun 18, 2012 4:10 pm
Forum: Techniques and Tools
Topic: Pattern Bar/Devit question
Replies: 4
Views: 9469

Pattern Bar/Devit question

I made a sushi platter from pattern bars. Some of the cuts were thicker than others. Prior to firing the piece it had an uneven surface, it didn't fuse totally flat and has some devit. Would it have been better to increase the temp or increase the hold.(For the flatter surface) ( BE glass 1807-1808-...
by Gail L
Sun Jun 03, 2012 9:53 am
Forum: Newcomer Forum
Topic: cutting circles
Replies: 14
Views: 41240

Re: cutting circles

Wrong...it IS deserved !
by Gail L
Sat Jun 02, 2012 10:34 am
Forum: Newcomer Forum
Topic: cutting circles
Replies: 14
Views: 41240

Re: cutting circles

I got your 51 months comment immediately Brock ! When I first started reading the board there were "posters" that I realized right away, knew what they were talking about....one of them being you. I have my very own "Brock Binder" that is filled with information and schedules. Pr...