Search found 2 matches
- Thu Jul 10, 2003 1:50 pm
- Forum: Kiln Casting
- Topic: shell inclusions
- Replies: 2
- Views: 7767
Dear Brad, sorry it took so long for me to get back to the Board. I am living, right now, at the beach in Costa Rica, and we' re experiencing telephone line difficulty. I tried to encase the sea shells with frit in a small frit casting square mold. It was five inches by five inches. The firing sched...
- Sat Jul 05, 2003 5:54 pm
- Forum: Kiln Casting
- Topic: shell inclusions
- Replies: 2
- Views: 7767
shell inclusions
I've done an experiment with bullseye frit 1101clear and seashells. The piece broke apart within 30 minutes of cooling it. Any info would be appreciated.
Thank you
Carol
Thank you
Carol