Search found 10 matches

by HEIDI in Wa. state
Tue Jun 25, 2013 11:54 pm
Forum: Techniques and Tools
Topic: latest and greatest kiln
Replies: 12
Views: 27047

Re: latest and greatest kiln

I agree with Brock. Keep an eye on Craigslist for them. I just picked up two from two different people for $800 ea with about $500 worth of glass a supplies!
HEIDI
by HEIDI in Wa. state
Mon Feb 18, 2013 8:16 pm
Forum: Community Projects
Topic: 2013 Magnet Exchange Now Underway
Replies: 50
Views: 869962

Re: 2013 Magnet Exchange Now Underway

Barbara Cashman wrote:Me too. My tests are not going well....
Mine either, I think I better come up with a plan B
HEIDI
by HEIDI in Wa. state
Sat Feb 16, 2013 1:05 am
Forum: Community Projects
Topic: 2013 Magnet Exchange Now Underway
Replies: 50
Views: 869962

Re: 2013 Magnet Exchange Now Underway

That's right it's getting close, Hmm, maybe I should think about starting.
HEIDI
by HEIDI in Wa. state
Tue Feb 12, 2013 2:21 pm
Forum: Techniques and Tools
Topic: Viewing windows in kilns
Replies: 8
Views: 21189

Viewing windows in kilns

I was wondering, are the viewing windows worth the extra money you pay for them? Anyone out there have one-feedback would be appreciated.
http://www.skutt.com/glass/accessories/window.php
Thanks,
HEIDI
by HEIDI in Wa. state
Wed Sep 12, 2012 10:30 pm
Forum: Techniques and Tools
Topic: how do i do this
Replies: 6
Views: 14435

Re: how do i do this

I didn't mean my comment to suggest you were going to copy, my statement was more a general one. Sorry if I offended you, I truly didn't mean too.
HEIDI
by HEIDI in Wa. state
Wed Sep 12, 2012 8:35 pm
Forum: Techniques and Tools
Topic: how do i do this
Replies: 6
Views: 14435

Re: how do i do this

Brad Walker wrote:It is not a good idea, nor is it legal, to copy someone else's design. Better to come up with your own design.
Thanks Brad, it is not my design either, but, for some reason we need to remind people of this sometimes...
HEIDI --who is having someone copy her designs right now....
by HEIDI in Wa. state
Thu Aug 30, 2012 3:41 pm
Forum: Techniques and Tools
Topic: Glass meant for shelves
Replies: 7
Views: 17730

Re: Glass meant for shelves

I was given some of this type of glass a few months ago. I did screen print on it. After it was fired, I sandblasted then slumped. Worked great. Still can't figure out the whole "tin side" thing. I would not have paid for the glass, but has been fun to play with.
by HEIDI in Wa. state
Mon Jul 02, 2012 1:38 pm
Forum: Photos and Stuff
Topic: Old Grinder
Replies: 6
Views: 15138

Re: Old Grinder

I bought one of those a few months ago as well! $5. at a swap meet. I love the small work area for smaller pieces. Mine of course doesn't look as nice as yours...
HEIDI
by HEIDI in Wa. state
Wed Jun 20, 2012 1:01 am
Forum: Techniques and Tools
Topic: Printing on thin fire
Replies: 6
Views: 18479

Re: Printing on thin fire

I have a print gocco silkscreen printer. Which brand of enamel paint would you recommend? is it hard to silkscreen on the glass? The logo would not be more then 2X 2 inches. also does the print need to be capped with clear 96? Thanks for sharing your expert knowledge Oh, those print Gocco units are...
by HEIDI in Wa. state
Tue Jun 19, 2012 12:53 pm
Forum: Techniques and Tools
Topic: Printing on thin fire
Replies: 6
Views: 18479

Re: Printing on thin fire

I just did a 200 piece trophy order. They also wanted their logo. I screen printed them and they looked great. If you don't have access to that option test the Thinfire method and just make the white a design element.
HEIDI