Kelly,

I have had a 28" by 15" by 1/4" Bullseye tabletop on my open poarch for two years. It is sitting atop a metal frame with bumpons to cushion it. It has survived temperatures from freezing to 100 degrees and three rambunctious grandchildren with no apparent damage.

Cecilia