Search found 18 matches

by Betty
Mon Jun 30, 2003 11:20 pm
Forum: Techniques and Tools
Topic: 90 coe and 96 coe Q
Replies: 1
Views: 4893

advice from a beginner

Take the glass coe 96 fires cooler than the coe 90 just don't mix up the glasses and mix the coe. When they come out of my kiln they all look Gooood. I fire with both and have them in seperate places in the shop.
by Betty
Sun Jun 29, 2003 5:27 pm
Forum: Techniques and Tools
Topic: New Skutt
Replies: 2
Views: 6619

after 12 years of stained glass the kiln has gotten me hooked on glass again. I used the pre programed programs with the skutt for a couple of weeks and then figured out how to set the kiln at different settings it is great fun each morning to see what comes out. If you changes the temp. besure to k...
by Betty
Sat Jun 28, 2003 9:43 pm
Forum: Techniques and Tools
Topic: Kiln Wash Off SS
Replies: 7
Views: 13779

Kiln Wash Off SS

I want to apply new wash to stainless steel. But the old won't wash off. it is streakie, not covered well in places and to much in other places. Should i steel wool it off and heat?
by Betty
Wed Jun 18, 2003 9:30 pm
Forum: Techniques and Tools
Topic: melt pot
Replies: 2
Views: 6261

Thank you, as soon as I get the supports to hold the pot i will do this.
by Betty
Wed Jun 18, 2003 9:25 pm
Forum: Techniques and Tools
Topic: Pot Melt Firing Schedule
Replies: 9
Views: 16583

melt pot

I am getting ready to try the melt pot thing. Let us know how it turn out.
by Betty
Tue Jun 17, 2003 3:23 pm
Forum: Techniques and Tools
Topic: melt pot
Replies: 2
Views: 6261

melt pot

I want to try the melt pot,

Do i need kiln wash on the melt pot (aka flower pot)? all these scarpes it is nice to use them up.
by Betty
Thu Jun 12, 2003 9:26 am
Forum: Techniques and Tools
Topic: Uroboros Glass Frit Mosaic
Replies: 4
Views: 8715

Thank You, better to ask and better to not take the chance

Thanks
Betty
by Betty
Wed Jun 11, 2003 6:02 pm
Forum: Techniques and Tools
Topic: Uroboros Glass Frit Mosaic
Replies: 4
Views: 8715

Uroboros Glass Frit Mosaic

Just got Uroboros glass frit Mosaic size, and it has a white powder or dust all over the glass pieces. Do I need to remove the dust from the pieces?

The glass i fired last night I cleaned with rubbing alocolce and it looked good this morning.

Betty
by Betty
Sun Jun 08, 2003 8:51 am
Forum: Techniques and Tools
Topic: COE for Most Armstrong and Youghiogeny Glass Question
Replies: 16
Views: 28398

youg. glass

I have slumped with youg. glass in a single sheet into a bulleye mold it has come out good the colors have changed and muddied a bit but for a candle holder it is ok.
by Betty
Thu May 01, 2003 8:29 pm
Forum: Techniques and Tools
Topic: How Hot?
Replies: 1
Views: 5620

How Hot?

The small, 4" & 6', molds have not slumped I reset the temp. to 1275 degrees. Hold time is 10 minutes

Just how hot can the mold go before they crack? The glass is only a single layer of fusing glass.
by Betty
Mon Apr 14, 2003 5:48 pm
Forum: Techniques and Tools
Topic: Where on the EAST coast to buy Bullseye and supplies?
Replies: 8
Views: 17474

Warner-crivellaro in allentown Pa is fast

http://WWW.Warner-Criv.com.

Do a search under 96-*

there are all kinds of things. the warm glass is only on the internet but they are putting out a new catologe soon.
by Betty
Sun Apr 13, 2003 10:47 am
Forum: Techniques and Tools
Topic: Why want it slump?
Replies: 8
Views: 16940

I would love to change the temp. but the direction are confussing to me. Going away for a week and will call Skutt when i get home.
by Betty
Sat Apr 12, 2003 9:00 pm
Forum: Techniques and Tools
Topic: Why want it slump?
Replies: 8
Views: 16940

Rate Soak Hold 400f/hour 600f 5 min 600f/hour by process by process 9999f/hour 960f 40 min 175f/hour 800f 10 min like i said it still makes no sence to me but it willl
by Betty
Sat Apr 12, 2003 8:53 pm
Forum: Techniques and Tools
Topic: Why want it slump?
Replies: 8
Views: 16940

It is a new kiln, skutt Hot start, and I am using the preprogramed settings. The insturation are confusing for me.

The firing was medium speed and slump with a soak of 1225 for 15 minutes

Just what all this means i am still learning.
by Betty
Sat Apr 12, 2003 8:33 pm
Forum: Techniques and Tools
Topic: Why want it slump?
Replies: 8
Views: 16940

Art Glass

What i am using in the stained art glass. I just want to slump it in some small molds.
by Betty
Sat Apr 12, 2003 4:35 pm
Forum: Techniques and Tools
Topic: Why want it slump?
Replies: 8
Views: 16940

Why want it slump?

I put one piece of glass, not the heat glass just regural glass, in the kiln and it didn't slump in the mold. Won't regural glass slump or does it need to be hotter to slump. there are just so many beautiful glass it seems a shame not to try a few.
by Betty
Fri Apr 04, 2003 12:16 am
Forum: Techniques and Tools
Topic: HELP it's stuck
Replies: 5
Views: 14020

It is a pours pottery mold in the shape of a drinking glass. 5.5" tall and in the freezer at the moment. idea from the place i by the molds.

I was thinking about trying to make another mold using this mold as a shape, guess i need to find out how to make molds.

Betty
by Betty
Wed Apr 02, 2003 10:51 pm
Forum: Techniques and Tools
Topic: HELP it's stuck
Replies: 5
Views: 14020

HELP it's stuck

First slump and the glass is stuck to the mold. I kilned washed it and let it dry 2 days and the glass is stuck.

I have put it in water to soak is there anything else i can do?

Betty