Re: Lamp worked rondels and other 2D forms
... It's a pain in the neck to arrange a bunch of (probably jagged-bottomed) stringer or rod or cane--they want to fall over. I typically cut some strips of scrap about a half-inch wide, interleave them to make a frame that's slightly thinner than the length of the pieces. Then I stand the kilnshel...
- Sat Sep 06, 2014 1:54 am
- Forum: Photos and Stuff
- Topic: Combing with Reactives
- Replies: 23
- Views: 69375
Re: Combing with Reactives
exquisite

- Thu Jul 24, 2014 3:23 am
- Forum: Newcomer Forum
- Topic: BE 0146 Steel Blue - powder
- Replies: 5
- Views: 21201
Re: BE 0146 Steel Blue - powder
I want the opposite - if I use the steel blue powder uncapped will I get silver color where the powder is - even if it is a tiny line?
- Thu Jul 24, 2014 3:22 am
- Forum: Newcomer Forum
- Topic: Big bubbles on flat fuse
- Replies: 8
- Views: 35492
Re: Big bubbles on flat fuse
definitely measure - using the brush I use the 10 to one measurement when I use my air compressor to spray my shelves I use 20 to one and I don't really count how many layers I just look for an even coating of pink. I used to spray all the time. When I brush it's because I'm being lazy. But the firs...
- Tue Jul 22, 2014 2:07 pm
- Forum: Business Topics
- Topic: and I thought the economy was bad
- Replies: 3
- Views: 17880
Re: and I thought the economy was bad
who is the distributor?
- Tue Jul 22, 2014 2:05 pm
- Forum: Newcomer Forum
- Topic: Big bubbles on flat fuse
- Replies: 8
- Views: 35492
Re: Big bubbles on flat fuse
bubble on kiln wash seem to appear only if the kiln wash is too thick. I mix 10 to 1 and only use one or 2 coats over an existing layer. After the kilns wash shows wears I scrape and start over again with maybe 3 layers. hope this helps.
- Fri Jul 18, 2014 1:54 am
- Forum: Techniques and Tools
- Topic: does dichroic stand up in a pot melt?
- Replies: 4
- Views: 10894
Re: does dichroic stand up in a pot melt?
post it to ebay or craig's list someone will buy small pieces I would hate to see dichro burn.
- Fri Jul 18, 2014 1:50 am
- Forum: Photos and Stuff
- Topic: my best glass story
- Replies: 8
- Views: 32095
my best glass story
This might be the best story of my glass career. I was selling at the Palo Alto Clay and Glass Festival this past weekend. Of course I had my glass portraits with me. They are my higher end items and so people take a little time to think about it. It just so happened that I had so quite a few the sh...
- Tue May 20, 2014 6:57 pm
- Forum: Business Topics
- Topic: Donations/Pricing
- Replies: 14
- Views: 43060
Re: Donations/Pricing
luckily the retail value of the item was only 45.00 - I don't put myself out there very much....Marty wrote:Terry- the answer is no. You can add "sorry" if you like but I wouldn't. You put yourself out enough.
- Tue May 20, 2014 6:37 pm
- Forum: Business Topics
- Topic: Customers Asking for Discounts
- Replies: 19
- Views: 71106
Re: Customers Asking for Discounts
I just say that I'm an hones person and I don't play games with fluctuating prices. Plus most of my work is one of a kind. I find it totally confusing to have one set of price and selling for another. The most I will do is I have certain items already marked 1 for 30 or 2 for 55.00. Or I may pay tax...
- Wed May 07, 2014 1:54 am
- Forum: Business Topics
- Topic: Donations/Pricing
- Replies: 14
- Views: 43060
Re: Donations/Pricing
I got asked to donate to an organization that I used to do a lot of award for and I had a personal connection with the director. The director is gone so I'm not as connected. When the director retired I gave them a 1200.00 piece for 300.00 I wanted to because I have decades of respect for this direc...
- Sun May 04, 2014 1:36 am
- Forum: Business Topics
- Topic: Donations/Pricing
- Replies: 14
- Views: 43060
Re: Donations/Pricing
I think you can only count the cost of materials as the amount donated - mind you this is a slippery slope.
- Sun May 04, 2014 1:34 am
- Forum: Techniques and Tools
- Topic: adjusting sheet glass to fit my needs
- Replies: 14
- Views: 25207
Re: adjusting sheet glass to fit my needs
Working outside your kiln, you could set up an uncoated silk screen frame and 'squeegee' on layers of colors until your desired color is achieved. Where do you buy your uncoated screens - :?: someone gave me a name of a company but they only do wholesale - I would not be buying enough to establish ...
- Mon Apr 28, 2014 5:04 pm
- Forum: Newcomer Forum
- Topic: Irid Food Safe?
- Replies: 9
- Views: 29767
Re: Irid Food Safe?
Yes it can go into the dishwasher but do you normally put art into the dishwasher? Then if that doesn't work I tell them that when you put things in the dishwasher all your plates are the same and so when they move around they do it in unison - if you have an shape that doesn't match all the other p...
- Fri Apr 25, 2014 12:54 am
- Forum: Business Topics
- Topic: photos showing up in IE and FIrefox but not Chrome
- Replies: 1
- Views: 11577
photos showing up in IE and FIrefox but not Chrome
I spent a ton of time using mailchimp to do my beginning of the year announcement. then when I test it to send to different mail address - yahoo,.gmx,gmail pictures show up in gmail using chrome but not in yahoo or gmx. If I use IE the pictures show up in yahoo, gmail and gmx. I emailed mail chimp b...
- Sun Apr 20, 2014 9:12 pm
- Forum: Jewelry Making
- Topic: belt buckle blanks
- Replies: 5
- Views: 161101
- Fri Mar 21, 2014 10:27 pm
- Forum: Techniques and Tools
- Topic: photo decals - black and white
- Replies: 2
- Views: 7747
Re: photo decals - black and white
Best I can tell, this is the standard decal paper available in many places including our web store (see below). Many canon printers do have the iron oxide in the toner, but some do not. You are pretty safe with HP black only printer Note: you still get the "sepia" color, also known as rus...
- Thu Mar 20, 2014 10:03 pm
- Forum: Techniques and Tools
- Topic: photo decals - black and white
- Replies: 2
- Views: 7747
photo decals - black and white
Hand any one used photo decals from Fusion? http://www.fusionheadquarters.com/product_p/decpap.htm
It says"If your printer is a Black and White HP or Canon Laser Printer or copier and has absolutely NO capability of printing in color… it will work."
Thanks -
It says"If your printer is a Black and White HP or Canon Laser Printer or copier and has absolutely NO capability of printing in color… it will work."
Thanks -
- Sun Feb 02, 2014 7:41 pm
- Forum: Business Topics
- Topic: website listing submissions
- Replies: 2
- Views: 14995
Re: website listing submissions
thanks!!!
- Sun Feb 02, 2014 1:58 am
- Forum: Business Topics
- Topic: website listing submissions
- Replies: 2
- Views: 14995
website listing submissions
I have to make some quickie websites for some friends for open studios in May. I can't seem where to submit my new website addresses so that they appear when searched by Google or other search engine. Long long time ago I remember you could just go to Google or yahoo and submit a url. Of course I wo...