by sallie4str
Tue Mar 18, 2003 3:08 pm
Forum: Techniques and Tools
Topic: Silver Clay and Glass Molds
Replies: 6
Views: 14904

Silver Clay and Glass Molds

Has anyone used silver clay inside glass?
Is it even possible?
The COE of Silver is 191, is it possible to layer the glass on either side of the silver and give the illusion of encasement?
I am going for a concept, any ideas are welcome?
:?