Search found 28 matches
- Mon May 12, 2003 12:31 am
- Forum: Techniques and Tools
- Topic: Wierd tingling in fingers after grinding and sawing
- Replies: 20
- Views: 28262
I have carpal tunnel and have found that wearing wrist braces when doing activities that put stress on wrists really helps...although I agree that this doesn't sound like it probably is. But for those that do have signs of it I have found that the kind of braces that don't have the metal shaft in th...
- Sat May 10, 2003 9:01 pm
- Forum: Techniques and Tools
- Topic: wasser glass yucky!
- Replies: 7
- Views: 9105
I bought quite a bit of Wasser several years ago when they went out of business, including the perferated glass, only to find that I had compatability problems when I combined it with Bullseye in larger pieces. It works fine when combined for jewelry or other smaller works. I have tried running test...
- Sun Apr 27, 2003 11:40 pm
- Forum: Techniques and Tools
- Topic: Fixing Sagging Elements
- Replies: 15
- Views: 18072
- Thu Apr 24, 2003 12:32 pm
- Forum: Business Topics
- Topic: cost of studio help
- Replies: 8
- Views: 11658
- Fri Mar 28, 2003 1:30 am
- Forum: Techniques and Tools
- Topic: stupid person with a stupid problem
- Replies: 8
- Views: 11384
- Fri Mar 28, 2003 1:26 am
- Forum: Techniques and Tools
- Topic: stupid person with a stupid problem
- Replies: 8
- Views: 11384
After having a catastrophic melt down due to a malfunction of my Kilntrol kiln controller I now never trust one even though I have replaced it with a Barton which has worked fine so far. I had a kiln sitter put on my kiln and now always use it as a back up. I use a cone that is a little hotter than ...
- Sat Mar 22, 2003 2:55 am
- Forum: Techniques and Tools
- Topic: Tack Fusing noodles during slump cycle
- Replies: 3
- Views: 6661
- Sat Mar 22, 2003 1:51 am
- Forum: Techniques and Tools
- Topic: Slumping Into A Wok
- Replies: 5
- Views: 9335
I have been slumping into a large steel wok because I couldn't find a large enough stainless one. So far no major problems except the kiln wash deteriorates with each firing and I must reapply. I have only used it 6 or 8 times tho so don't know long term. I use a scrubby and water to clean off the c...