Search found 13 matches

by Karyn Cott
Sat Feb 15, 2014 4:44 pm
Forum: Techniques and Tools
Topic: copper as a mold
Replies: 2
Views: 15339

Re: copper as a mold

Thanks for the confirmation Brock.
by Karyn Cott
Sat Feb 15, 2014 4:34 pm
Forum: Techniques and Tools
Topic: copper as a mold
Replies: 2
Views: 15339

copper as a mold

I have a copper "jello" mold that states it is solid copper. Can I use this as a casting mold?
by Karyn Cott
Wed Oct 02, 2013 6:37 pm
Forum: Techniques and Tools
Topic: this is for Bert
Replies: 1
Views: 4687

this is for Bert

Hi Bert, Many years ago you gave me a float glass fusing schedule for three 2 mm sheet glass (total 6 mm). I cannot find it anywhere and would appreciate you giving it to me again please. I always use BE glass but have come across a great amount of float glass and wish to use it. And you also told m...
by Karyn Cott
Mon Jul 22, 2013 6:45 pm
Forum: Techniques and Tools
Topic: cast iron
Replies: 0
Views: 21259

cast iron

Can cast iron be used in fusing or would it spall too much :?:
by Karyn Cott
Mon Feb 25, 2013 11:25 am
Forum: Techniques and Tools
Topic: steel rod
Replies: 5
Views: 9730

Re: steel rod

Thanks for the info. I just wanted a ball park answer so I could start experimenting myself. I have a small wooden chair that I want to make a glass blanket for. The blanket might just be woven rod or stringer or 1/4 inch fused glass; I have not made up my mind yet, I am wanting to drape this blanke...
by Karyn Cott
Mon Feb 25, 2013 11:18 am
Forum: Techniques and Tools
Topic: slumping glass into a glazed ceramic mold
Replies: 10
Views: 24091

Re: slumping glass into a glazed ceramic mold

I use Universal Mold Coat that Boyce Lundstrum developed. You add acrylic paint to the powder mixture and it lasts through several firings. No need to scuff the surface and it leaves the back of the piece very smooth. I love the product.
by Karyn Cott
Sun Feb 24, 2013 9:24 pm
Forum: Techniques and Tools
Topic: steel rod
Replies: 5
Views: 9730

steel rod

I want to bend glass over steel rod. My question is this: How thick should the rod be before it will bend and how high of a temperature can I go before it will bend? :?:
by Karyn Cott
Thu Nov 29, 2012 3:41 am
Forum: Techniques and Tools
Topic: rigidizing fiber blanket
Replies: 9
Views: 18084

Re: rigidizing fiber blanket

Thanks for your input Cynthia; it is appreciated. Bert, sand does sound like a mess so perhaps just some extra rolled up fiber blanket will be enough to support the curved ends? What do you think?

K
by Karyn Cott
Tue Nov 27, 2012 10:10 pm
Forum: Techniques and Tools
Topic: rigidizing fiber blanket
Replies: 9
Views: 18084

Re: rigidizing fiber blanket

Thank you Bert; I had thought of using sand for the entire mold but my "techie" said sand would not work. I have casted onto sand before and loved the results. I will take your advice and prop up the mold with bricks or sand to dry it in the kiln and leave it that way when I slump the long...
by Karyn Cott
Tue Nov 27, 2012 8:41 pm
Forum: Techniques and Tools
Topic: rigidizing fiber blanket
Replies: 9
Views: 18084

rigidizing fiber blanket

I think I was given some bum advice. I needed to make a mold that was 7" x 24" for a special order piece. All it needed to be was like a long and narrow sushi plate. I just needed a slight up-curve on the ends. I was told to get thick fiber blanket and soak it with rigidizer and let it dry...
by Karyn Cott
Thu Oct 11, 2012 7:43 pm
Forum: Techniques and Tools
Topic: Firing glass over plant material
Replies: 6
Views: 11194

Re: Firing glass over plant material

When I use foliage under glass, I will cut the thick parts lengthwise and I also either dry them flat with weight on them or I put them in the microwave with weight and dry them out that way. With this method I have never had an issues with bubbles or breakage. I have done this many times and have s...
by Karyn Cott
Tue Jun 26, 2012 7:27 pm
Forum: Techniques and Tools
Topic: boron nitride
Replies: 3
Views: 6899

Re: boron nitride

One other question. I am draping over a ss form for a lamp shade. I want somewhat of a texture to the inside so that the light from the bulb is diffused. Would it work if I draped fiber blanket (that I separate into a thinner piece) over the ss form?
by Karyn Cott
Tue Jun 26, 2012 6:48 pm
Forum: Techniques and Tools
Topic: boron nitride
Replies: 3
Views: 6899

boron nitride

I have a can of boron nitride and was wondering if you all like to use it on stainless steel or do you feel that kiln wash works better?