I once made cookie cutters out of brass for my boss (whale shapes). She was surprised. I found a stainless steel sheet at Lowes. It was a back splash for the wall between the kitchen stove and overhead vent(I don't know what it is called). It's thin enough to cut strips with a paper cutter to a vari...