- Mon Jan 14, 2013 7:13 am
- Forum: Techniques and Tools
- Topic: annealing 96 question
- Replies: 8
- Views: 11491
Re: annealing 96 question
thanks Barb, that makes sense... my thinking was stuck in a groove... I thought I had the correct firing prog from when I did this about a year ago but I must have lost the right page with the longer program from my folder. It just didn't connect with my brain that the anneal soak was too short. (No...
- Sat Jan 12, 2013 3:14 am
- Forum: Techniques and Tools
- Topic: annealing 96 question
- Replies: 8
- Views: 11491
Re: annealing 96 question
1/2"(12mm) thick, 12" ( 30cm) round. Slump ( into sand) prog was: Farenheit; 300/1000/20 570/1380/60 AFAP/1000/45 75/970/90 75/900/15 130/750/10 Celcius; 150/540/20 300/750/60 AFAP/540/45 25/520/90 25/485/15 55/400/10 I thought this ramp down would be slow enough to anneal but seems not. 2...
- Fri Jan 11, 2013 6:01 pm
- Forum: Techniques and Tools
- Topic: annealing 96 question
- Replies: 8
- Views: 11491
Re: annealing 96 question
25 degreesC (77F ) be slow enough?
- Fri Jan 11, 2013 5:39 pm
- Forum: Techniques and Tools
- Topic: annealing 96 question
- Replies: 8
- Views: 11491
annealing 96 question
hypothetically , if a project was not sufficiently annealed, is it possible to reheat to anneal temp and redo the anneal ?
thanks Stef