Bert,
If Klyn-fire is mae with CMC and it tastes good, do you want the receipt that makes the klyn-fire taste good.. or just the one with good taste.
Stuart
Search found 224 matches
- Thu Apr 01, 2004 2:41 pm
- Forum: Techniques and Tools
- Topic: CMC vs. Kylr-Fire
- Replies: 6
- Views: 11581
- Thu Apr 01, 2004 12:36 pm
- Forum: Techniques and Tools
- Topic: When looking for a used kiln
- Replies: 4
- Views: 5919
- Thu Apr 01, 2004 11:44 am
- Forum: Techniques and Tools
- Topic: Duraboard repair
- Replies: 8
- Views: 9693
- Tue Mar 30, 2004 2:26 pm
- Forum: Techniques and Tools
- Topic: artists/studios/museums in ireland?
- Replies: 14
- Views: 17407
There is a crafts council with branches in Dublin and Kilkenny. In Kilkenny there were a few studios/galleries to talk thru for all type of crafts. Near Kilkenny (which has a nice castle also) is Jerpoint Crystal. There is an outlet in town and they can give you directions and a brouchure about the ...
- Mon Mar 29, 2004 9:03 pm
- Forum: Techniques and Tools
- Topic: artists/studios/museums in ireland?
- Replies: 14
- Views: 17407
Second the waterford part. I will have to do some homework, but close to the ring of Kerry I found a Hot glass artist that used old green coke bottles for his batch or cullet. Everything he does is green, but that is ok since you are in Ireland. There also is another place, south of Dublin, before w...
- Mon Mar 29, 2004 2:20 pm
- Forum: Techniques and Tools
- Topic: welding cloth on walls
- Replies: 5
- Views: 9187
Ron, Cute little guy there sipping coffee.... so, now we know about your job, you think about how to enginner your next project (glass one, not work one), and you sit there reading the paper, plans and this board. I have been trying to talk Jim into coming to WGW... he won't. I guess you will jsut h...
- Mon Mar 29, 2004 1:53 pm
- Forum: Techniques and Tools
- Topic: Hey Dick . . .
- Replies: 26
- Views: 39263
- Sun Mar 28, 2004 11:16 pm
- Forum: Techniques and Tools
- Topic: Lessons Learned . . .
- Replies: 25
- Views: 34344
Paul, It is interesting.. Since I started repairing the kilns I was told that most of the times the relays break in the open position and they will not work. But I have replaced more of them with the relays that are stuck closed and keep firing even when the controller is not telling it to fire. Eve...
- Sun Mar 28, 2004 12:23 pm
- Forum: Techniques and Tools
- Topic: Paragon Kiln help and question on 3 key controller
- Replies: 7
- Views: 7462
- Sun Mar 28, 2004 12:21 pm
- Forum: Techniques and Tools
- Topic: Lessons Learned . . .
- Replies: 25
- Views: 34344
Ok, I need to explain something.. Brock understand but I got a few e-mails from others about what I wrote. What Brock was suggesting was to use the controller normally. In case there was a problem use a cone that would bend and trip the setter only if the temp got hotter and for a longer time. Hopef...
- Sun Mar 28, 2004 11:22 am
- Forum: Techniques and Tools
- Topic: Lessons Learned . . .
- Replies: 25
- Views: 34344
- Sun Mar 28, 2004 11:08 am
- Forum: Techniques and Tools
- Topic: Lessons Learned . . .
- Replies: 25
- Views: 34344
Brock, I would think that the concern would be time. But if the concern is that a slump firing or tack firing gets to hot then each time there is a different type of firing the cone would be changed. Also, the installation would be harder since besides hooking up the electrical part a hole would be ...
- Sun Mar 28, 2004 10:53 am
- Forum: Techniques and Tools
- Topic: Lessons Learned . . .
- Replies: 25
- Views: 34344
You can add kilnsetter to your kiln. Basically you want the timer part added, where if you go over your estimated time for a firing it will shut it off. You will be basically be adding it on to one of your wires. but do you really think it is necesary.. If one of your relays breaks in the closed pos...
- Sun Mar 28, 2004 10:38 am
- Forum: Techniques and Tools
- Topic: Paragon Kiln help and question on 3 key controller
- Replies: 7
- Views: 7462
Which 3 key controller is it? Paragon sold 2. In the past it was the Bartlett board, now it is the Orton. I am a Paragon Certified repair person (That certificate and 10¢ still will not buy me a cup of coffee), but have the person drop me an e-mail with what the code is and then I can get them what...
- Sat Mar 27, 2004 11:25 pm
- Forum: Techniques and Tools
- Topic: glass cuttimg medium
- Replies: 51
- Views: 54969
- Sat Mar 27, 2004 10:05 pm
- Forum: Techniques and Tools
- Topic: black magic
- Replies: 13
- Views: 12495
- Sat Mar 27, 2004 9:40 pm
- Forum: Techniques and Tools
- Topic: black magic
- Replies: 13
- Views: 12495
the product is back magic, but there is black magic involved... the black magic part is that the prodcut is still sold.. and they we have nto run them out of town on the rail... The product does not work.. I even called the manufacturer and the woman that answer the phone told me not to use it but t...
- Tue Mar 23, 2004 7:22 pm
- Forum: Techniques and Tools
- Topic: kiln brick repair ?? after overheating
- Replies: 9
- Views: 10716
I would forget the patch and just put a shelf over the hole. The patch is good to glue back parts of the brick in a whole. If you put a large glob of it, it will just eventually pop out. You must dig the glass out. The glass will erode out the brick. For future reference.. put kiln wash on the botto...
- Tue Mar 23, 2004 7:17 pm
- Forum: Techniques and Tools
- Topic: Help with a slump and crack...newbie..
- Replies: 9
- Views: 11174
7 layers.. the problem might not be that you pulled it out, but that it was not annealed enough. You need to go very slow on the ramp up.... and if you question if the speed you want to go is slow enough it is not, go slower. There is a LARGE chance that it will crack on the way up if it was not ann...
- Tue Mar 23, 2004 7:00 pm
- Forum: Techniques and Tools
- Topic: kiln brick repair ?? after overheating
- Replies: 9
- Views: 10716
The glass will keep eating away at the brick. Remove the glass before you patch the whole. The problem with the cement is the the brick and cement might expand at different rates. Unless the bottom of the kiln is showing when you remove the glass it might not need to be repaired. Can you put a shelf...