Search found 7 matches
- Sat Dec 19, 2015 1:17 pm
- Forum: Techniques and Tools
- Topic: The piece that haunts me.... (pic)
- Replies: 2
- Views: 4714
The piece that haunts me.... (pic)
We all have one, right? The piece that was sold or given away as a gift, that you continue to think about and wish you had back? Mine might inspire some of you, way more talented than I, to refine this technique. So, I was experimenting with thick drops to make pendant lights. I didn't like one of m...
- Sat Dec 19, 2015 1:00 pm
- Forum: Techniques and Tools
- Topic: Thermal shock problem, first time in 12 years, pics
- Replies: 12
- Views: 16281
Re: Thermal shock problem, first time in 12 years, pics
Hi Bert, Thank you very much for your comments. You are right, any time the kiln is running unnecessarily it's a huge waste on multiple levels. Annealing at a lower temp makes a lot of sense given the mass of thicker glass. I will study more about this. I've seen you guys recommend the Graham Stone ...
- Fri Dec 18, 2015 5:40 pm
- Forum: Techniques and Tools
- Topic: Thermal shock problem, first time in 12 years, pics
- Replies: 12
- Views: 16281
Re: Thermal shock problem, first time in 12 years, pics
After a 26-hour firing cycle, I took a peek (at 175 degrees)...it looks like perfection, just tiny tiny bits of devit since this is the 5th firing. Given the mass, I will wait for further cooling before opening for a new picture. It's a Christmas Miracle! Thanks everyone.
- Thu Dec 17, 2015 3:33 pm
- Forum: Techniques and Tools
- Topic: Thermal shock problem, first time in 12 years, pics
- Replies: 12
- Views: 16281
Re: Thermal shock problem, first time in 12 years, pics
Thanks Valerie, I used Colorado Custom Stainless (303.433.2370). They made me a ton of different size casting rings, square, round, star--they would probably be able to do any type of shape (a fish shape would be cool!). Nice heavy gauge. I was able to give them dimensions of what I needed. It goes ...
- Thu Dec 17, 2015 1:47 pm
- Forum: Techniques and Tools
- Topic: Thermal shock problem, first time in 12 years, pics
- Replies: 12
- Views: 16281
Re: Thermal shock problem, first time in 12 years, pics
Marty....you were very observant, thank you! There is indeed a very thick layer of kiln wash adhered to the star legs...the thickest coatings are where the cracks started. I've ground off all the wash and am re-firing right now with your recommended changes to the schedule. I'll update tomorrow, tha...
- Thu Dec 17, 2015 11:56 am
- Forum: Techniques and Tools
- Topic: Thermal shock problem, first time in 12 years, pics
- Replies: 12
- Views: 16281
Re: Thermal shock problem, first time in 12 years, pics
It's my own schedule, I should have just put in 3:00 but it's my rush to get close to 3 hours (programming the rampmaster) and what's a few extra minutes. Why does the up-speed matter when the cracking is happening on the downside? Thanks
- Wed Dec 16, 2015 11:14 pm
- Forum: Techniques and Tools
- Topic: Thermal shock problem, first time in 12 years, pics
- Replies: 12
- Views: 16281
Thermal shock problem, first time in 12 years, pics
Hi Everyone! I've been a fusing hobbiest for over 12 years, this is my very first thermal shock issue that I'm trying to solve. My kiln is a 12-year old Evenheat, it has been a total steady eddy...absolutely no problems at all. It has about 500 hours of firing time I would guess, with nothing done o...