Hello people
i am interested in purchasing a disc grinder to use with different grits until to polish with pumice and/or cerium
What about your experience to suggest me a good tool?
thanks for support and collaboration
mike
Search found 67 matches
- Mon Sep 10, 2018 3:27 pm
- Forum: Techniques and Tools
- Topic: coldworking disc grinder
- Replies: 1
- Views: 7997
- Wed May 02, 2018 7:12 pm
- Forum: Kiln Casting
- Topic: Carving vermiculite
- Replies: 1
- Views: 35908
Carving vermiculite
Hi guys
anybody of you use to carve Vermiculute boards by hand or cnc router to make molds?
I would appeciete any reply
Thank you.
anybody of you use to carve Vermiculute boards by hand or cnc router to make molds?
I would appeciete any reply
Thank you.
- Wed May 02, 2018 7:08 pm
- Forum: Techniques and Tools
- Topic: Advice for a new kiln
- Replies: 0
- Views: 194887
Advice for a new kiln
Hello Guys
I d like to experiment pulling glass rods
Which glass kiln do you suggest?
Thanks for support
Mike ciao
I d like to experiment pulling glass rods
Which glass kiln do you suggest?
Thanks for support
Mike ciao
- Mon Apr 30, 2018 2:22 pm
- Forum: Techniques and Tools
- Topic: paragon window
- Replies: 3
- Views: 9974
Re: paragon window
Hi
Thank you.
I used thinfire paper of bullseye..and you are right.. Maybe was the fumes not vented.
It was not easy to clean but i did in the end.
So in which case i have to vent the kiln? And how?
(My paragon has a cone on the top?)
Thanks for your support and collaboration
Mike
Thank you.
I used thinfire paper of bullseye..and you are right.. Maybe was the fumes not vented.
It was not easy to clean but i did in the end.
So in which case i have to vent the kiln? And how?
(My paragon has a cone on the top?)
Thanks for your support and collaboration
Mike
- Wed Apr 25, 2018 5:38 am
- Forum: Techniques and Tools
- Topic: paragon window
- Replies: 3
- Views: 9974
paragon window
Hello friends,
during a fusing the window of my paragin sc2 with door and window become black and i am not able to see inside anymore?
what do you think happened?..and any way to restore the glass to look again inside?
thanks for support and collaboration,
mike
during a fusing the window of my paragin sc2 with door and window become black and i am not able to see inside anymore?
what do you think happened?..and any way to restore the glass to look again inside?
thanks for support and collaboration,
mike
- Wed Dec 27, 2017 7:45 am
- Forum: Techniques and Tools
- Topic: infrared termometer gun
- Replies: 0
- Views: 118342
infrared termometer gun
Hello People
i could be interested in purchasing this tool to read upside glass temperature while in the kiln.
Any suggest which one to buy?
Any help will be appreciate
thanks in advance
mike
i could be interested in purchasing this tool to read upside glass temperature while in the kiln.
Any suggest which one to buy?
Any help will be appreciate
thanks in advance
mike
- Sun Sep 24, 2017 12:08 pm
- Forum: Techniques and Tools
- Topic: edge fire polishing
- Replies: 4
- Views: 13563
Re: edge fire polishing
Hello people Thank you for your replies My.schedule is 0-550 30 min 550 soak 15min 550-690 asap 690 30 min. 690-750 asap Stop I also tried to brush The edges with spray A but nothing After cutting with saw i also try to use grind with a b dry belt to get less rough but nothing Any help? Thank you Mike
- Fri Sep 22, 2017 11:48 am
- Forum: Techniques and Tools
- Topic: edge fire polishing
- Replies: 4
- Views: 13563
edge fire polishing
Hello people I have troubles in edge fire polishing I use murano glass. I make plates in first firing, then i cut in small pieces with dish saw and the edge stay rough Then i need to firepolish the edge in a new firing I tried some times but the edges stay opaque? Maybe any help from antidevit on th...
- Sun Feb 12, 2017 1:46 pm
- Forum: Techniques and Tools
- Topic: deep texturing in sanblasting ?
- Replies: 4
- Views: 13125
Re: deep texturing in sanblasting ?
hi and thank you both for your help
In my opinion i think it is better for me first sancarving areas and then put in hide animal glue to create glue cjipping effect in the groove
thank you for support and collaboration
mike
In my opinion i think it is better for me first sancarving areas and then put in hide animal glue to create glue cjipping effect in the groove
thank you for support and collaboration
mike
- Sat Feb 11, 2017 2:10 pm
- Forum: Techniques and Tools
- Topic: polishing
- Replies: 4
- Views: 15178
Re: polishing
Hi
thanks for reply
i meant "edge" 6mm flat glass
what do you think?
thanks
mike
thanks for reply
i meant "edge" 6mm flat glass
what do you think?
thanks
mike
- Sat Feb 11, 2017 2:06 pm
- Forum: Techniques and Tools
- Topic: deep texturing in sanblasting ?
- Replies: 4
- Views: 13125
deep texturing in sanblasting ?
Hello People I have seen some glass made in a way i honestly i dindnt understand how they was made. I will show you some fotos and my idea. So in my idea i think that there is an surface etching ok, then the part we see shine and textured i think can be a sandcarved area then put somethinng in (like...
- Fri Oct 21, 2016 2:16 pm
- Forum: Techniques and Tools
- Topic: polishing
- Replies: 4
- Views: 15178
polishing
Hello friends
i have a question
What is best way to polish to get shine glass ? (firepolish?cerium?spray a o borax or something else?)
thanks for support and collaboration
ciao
i have a question
What is best way to polish to get shine glass ? (firepolish?cerium?spray a o borax or something else?)
thanks for support and collaboration
ciao
- Thu Oct 20, 2016 10:49 pm
- Forum: Kiln Casting
- Topic: glass castings into molds
- Replies: 2
- Views: 15559
Re: glass castings into molds
Thank you
What is best separator to get "shine" glass? is it also possible BN both on vermiculite or board?
thanks
mike
What is best separator to get "shine" glass? is it also possible BN both on vermiculite or board?
thanks
mike
- Thu Oct 20, 2016 2:53 pm
- Forum: Kiln Casting
- Topic: glass castings into molds
- Replies: 2
- Views: 15559
glass castings into molds
Hello friends
I am trying to carve hardnered fiber board and vermiculite to use for glass casting.
Are these the proper material to do this ?
What are best suggested separator to use with them?
thanks in advace for support and collaboration
mike from italy
I am trying to carve hardnered fiber board and vermiculite to use for glass casting.
Are these the proper material to do this ?
What are best suggested separator to use with them?
thanks in advace for support and collaboration
mike from italy
- Mon Feb 23, 2015 1:45 pm
- Forum: Newcomer Forum
- Topic: graphite
- Replies: 4
- Views: 17701
graphite
Hi.
i would like to know how to cut Grafite Plates.
thank you
mike
i would like to know how to cut Grafite Plates.
thank you
mike
- Mon Feb 23, 2015 1:44 pm
- Forum: Newcomer Forum
- Topic: murrine cutting machine
- Replies: 8
- Views: 36889
Re: murrine cutting machine
i hope to find it 
thank you
thank you
- Mon Feb 23, 2015 3:06 am
- Forum: Techniques and Tools
- Topic: vermiculite board for casting molds
- Replies: 15
- Views: 32846
Re: vermiculite board for casting molds
Hi thanks for reply
sent an email
sent an email
- Mon Feb 23, 2015 3:05 am
- Forum: Newcomer Forum
- Topic: murrine cutting machine
- Replies: 8
- Views: 36889
Re: murrine cutting machine
thank you fior your replies
I am looking for an automatic device.
DonMcClennen where to find BE video?
thabk you
mike
I am looking for an automatic device.
DonMcClennen where to find BE video?
thabk you
mike
- Sun Feb 22, 2015 5:57 pm
- Forum: Newcomer Forum
- Topic: murrine cutting machine
- Replies: 8
- Views: 36889
murrine cutting machine
Hi
i have a lot of Whole Murrina canes and i would like to build a device that cut they.
Any help?
thank you
i have a lot of Whole Murrina canes and i would like to build a device that cut they.
Any help?
thank you
- Sat Feb 21, 2015 4:01 pm
- Forum: Techniques and Tools
- Topic: glue for fiber boards
- Replies: 0
- Views: 21059
glue for fiber boards
hello people
i would like ask if exists any glue to fix fiber boards
thank for support
mike
i would like ask if exists any glue to fix fiber boards
thank for support
mike