Search found 7 matches
- Thu Apr 11, 2013 7:38 am
- Forum: Newcomer Forum
- Topic: Las Vegas Glass Expo
- Replies: 17
- Views: 42982
Re: Las Vegas Glass Expo
My class was disappointing. Instructor very unorganized and not enough supplies. I enjoyed the exhibit hall.
- Wed Apr 10, 2013 7:04 am
- Forum: Techniques and Tools
- Topic: textured glass bowl
- Replies: 2
- Views: 5440
textured glass bowl
Does anyone know where to buy textured glass cuboids or nuggets?
Thanks.
Thanks.
- Mon Apr 01, 2013 6:48 am
- Forum: Newcomer Forum
- Topic: Las Vegas Glass Expo
- Replies: 17
- Views: 42982
Re: Las Vegas Glass Expo
Tracy, this will be my first trip. I am taking a class by Janet Schrader. We get on Wed morning and stay thru Sunday. Am so looking forward to the whole experience!
- Thu Mar 28, 2013 6:30 am
- Forum: Newcomer Forum
- Topic: Las Vegas Glass Expo
- Replies: 17
- Views: 42982
Re: Las Vegas Glass Expo
I will be there.
Margaret Walker
Margaret Walker
- Wed Mar 06, 2013 7:55 am
- Forum: Techniques and Tools
- Topic: pendant light fixtures
- Replies: 5
- Views: 11196
Re: pendant light fixtures
Slumpy's has a large selection.
- Fri Feb 22, 2013 8:04 am
- Forum: Newcomer Forum
- Topic: Attaching a metal rod to Garden Art
- Replies: 15
- Views: 61457
Re: Attaching a metal rod to Garden Art
I drill a hole in the glass, then attach a copper tube to the glass using a screw and a washer. This has worked very well for me. Easy to assemble and disassemble for shipping purposes. Message me if you need further info.
- Mon Dec 17, 2007 12:33 pm
- Forum: Techniques and Tools
- Topic: signing name onto glass
- Replies: 3
- Views: 8329
signing name onto glass
Good morning all:
Besides etching your name onto glass, how are others signing your pieces? Is there a special pen to use after the piece has been fired?
Thanks.
Besides etching your name onto glass, how are others signing your pieces? Is there a special pen to use after the piece has been fired?
Thanks.