Search found 21 matches

by deena
Tue Nov 04, 2003 3:51 pm
Forum: Techniques and Tools
Topic: 1/2" From moving
Replies: 3
Views: 7035

It would be easier said than done. I will be damning tonight.
Thanks Deena

DC is only 3 hours from where I live. Thanks for the info.
by deena
Tue Nov 04, 2003 3:04 pm
Forum: Techniques and Tools
Topic: 1/2" From moving
Replies: 3
Views: 7035

1/2" From moving

I am making a table top that is 27 1/2 x 20 that has to fit within an 1/8" lip. Using 2 pieces of 1/4" glass airbrushed. I tried it firing to 1480 with lots of annealing time in between. The glass had a lot of movement and was to big. Do you have to dam the sides or can you fire it to a lo...
by deena
Wed Oct 15, 2003 9:21 am
Forum: Techniques and Tools
Topic: Glass Curtain
Replies: 19
Views: 32736

Cynthia, the curtain was beautiful. the connectors do not distract from you tiles.

Thanks for the information
Deena

(I forgot to put this in my last post, sorry)
by deena
Wed Oct 15, 2003 9:14 am
Forum: Techniques and Tools
Topic: Glass Curtain
Replies: 19
Views: 32736

Glass Curtain

It is 2 1/2' by 3 1/2'. thanks again for all of the great ideas. I will post a picture when I get it done.

Deena
by deena
Tue Oct 14, 2003 8:25 am
Forum: Techniques and Tools
Topic: Glass Curtain
Replies: 19
Views: 32736

Glass Curtain

I would like to do a glass curtain of 3x3 tiles on my bathroom window. Does anyone have any suggetions as what to use for connectors. I have tried wire wrapping but would prefer a cleaner look.

Thanks Deena
by deena
Fri Aug 29, 2003 7:33 am
Forum: Techniques and Tools
Topic: Float glass coated w/ dichroic
Replies: 5
Views: 10600

Bert,
Can you enamel and fuse the dicro in one step, then slump ,or do you have to do three fusings.

Thanks for the help

Deena
by deena
Thu Aug 28, 2003 1:03 pm
Forum: Techniques and Tools
Topic: Mica & float
Replies: 7
Views: 12454

Bert,

I would love to go to your class but cannot at the moment. If you plan on doing any more after dec in the area I would love to come. Virginia or North Carolina. My e-mail is deena@potteryglasscreations.com.
by deena
Tue Aug 26, 2003 11:39 am
Forum: Techniques and Tools
Topic: Mica & float
Replies: 7
Views: 12454

I meant sandwiching them between layers. Thanks for your help
Deena
by deena
Tue Aug 26, 2003 10:08 am
Forum: Techniques and Tools
Topic: Mica & float
Replies: 7
Views: 12454

Mica & float

I just recieved my new airbrush and am ready to try enamels and mica on float glass. After going thru the archives I am a little confused on firing pear-ex. Should you fire the blank (1/4" 2 layer first) Then the mica and use the slump firing for bonding the mica?And if you use enamels and mica...
by deena
Thu Aug 21, 2003 7:17 am
Forum: Techniques and Tools
Topic: Glass Tiles
Replies: 5
Views: 10089

Thanks for the info. That would help keeping the edges square. When I get a section done I will post a picture. The best thing is that after finding out what the costs of the tiles would have been at the tile store I can now tell my husband that "look honey the savings paid for the kiln" 8...
by deena
Wed Aug 20, 2003 12:00 pm
Forum: Techniques and Tools
Topic: Glass Tiles
Replies: 5
Views: 10089

I thought that it was not possible. The effect was great but I wondered about the mastic getting in between the glass eventually.

Thanks again
Deena
by deena
Wed Aug 20, 2003 9:00 am
Forum: Techniques and Tools
Topic: Glass Tiles
Replies: 5
Views: 10089

Glass Tiles

I have started making tiles to do the backsplash in my kitchen. I was at a tile store the other day and saw some wonderful 2x2 tiles. They were float glass with mica ans oxides and enamel. They were only tack fused together. The layer of enamels,ect were visible in between the 2 layers of glass. The...
by deena
Tue Jul 15, 2003 2:59 pm
Forum: Techniques and Tools
Topic: another drape question!
Replies: 4
Views: 8462

another drape question!

After having tried several times to drape a bowl I need help. I looked in the archives first but did not find an answer. The mold is ss about 12" in diameter. I am trying to get a lot of folds. Is thier anyway to cut the glass to make the folds more pronounced. Thanks for all of your help, past...
by deena
Wed Jul 09, 2003 8:55 am
Forum: Techniques and Tools
Topic: Drape question
Replies: 5
Views: 10458

Thanks for your help. This board has made my learing curve much easier.
Would a longer soak time make the folds more pronounced?

I am looking for very tight folds.

Thanks
Deena
by deena
Tue Jul 08, 2003 8:43 am
Forum: Techniques and Tools
Topic: Drape question
Replies: 5
Views: 10458

Drape question

Does anyone have any sugesstions for creating a very narrow 6 inch long drape. Can i use a very small ss measuring cup on top of kiln furniture? I may have posted this question twice. Sorry

Thanks Deena
by deena
Tue Jun 24, 2003 12:24 pm
Forum: Techniques and Tools
Topic: Unique paints
Replies: 3
Views: 6973

I have used these paints on float and go up to 1500. The red turned out fine. I tried an emerald green that turned almost clear. I called and they said to stir and shake and this would cure the problem. i have never tried airbrushing with them. :roll:

Deena
by deena
Thu Jun 05, 2003 12:47 pm
Forum: Techniques and Tools
Topic: kiln mishap
Replies: 7
Views: 14941

Thanks so much for the pictures and all of the help. Another project in the works. :P Deena
by deena
Tue Jun 03, 2003 1:04 pm
Forum: Techniques and Tools
Topic: kiln mishap
Replies: 7
Views: 14941

I wish I was not having this problem. Only having the kiln 3 weeks this was a disaster for me. The only thing I can think of is that the screw was not seated properly.

I am going to set up that pulley system. Thanks so much for your help
by deena
Tue Jun 03, 2003 10:12 am
Forum: Techniques and Tools
Topic: kiln mishap
Replies: 7
Views: 14941

kiln mishap

I just purchased an evenheat coffin kiln 13" deep. (3 weeks)The lid with elements is attached with 1-1" screw with chain on lid and same on body of kiln. I was nervous the first time i saw this and have been very gentle in opening the lid. WHile changing out the shelves the screw came out ...
by deena
Wed May 07, 2003 12:42 pm
Forum: Techniques and Tools
Topic: Slumping multiple pieces
Replies: 5
Views: 9137

Thanks for your help, IThis website has been a life saver... :P