Search found 4 matches

by nancyB inMD
Sun Mar 14, 2004 7:26 pm
Forum: Techniques and Tools
Topic: Shocking.....
Replies: 17
Views: 47030

There was a good discussion about metal cabinets , aluminum oxide and grounding on the sandcarvers group of yahoo several months back. I clipped the following, specifically about the wrist strap: "Current seeks the most direct path to ground. So if a spark does jump to an electrical wire it wil...
by nancyB inMD
Fri Jan 16, 2004 9:37 am
Forum: Techniques and Tools
Topic: Drilling holes in glass?
Replies: 6
Views: 24238

I have been using a corded Dremel with tripleripple bits for tiny holes. I need to make some holes i 1/8 inch in size and am not sure how well the Dremel will do the task or hold up to what I assume is more wear and tear and stress on the motor because of the size of the hole and thickness of the gl...
by nancyB inMD
Tue Oct 14, 2003 2:21 pm
Forum: Business Topics
Topic: waterproof my new canopy?
Replies: 8
Views: 20266

waterproof your canopy

There are several products in the camping section of *.*-mart that will help a lot in making your canopy water-resistant. "Camp Dry " is what I have. My KD is about 15 years old. I re-spray the canopy top every spring. It does not leak. There are a few small pin holes and they do drip in a...
by nancyB inMD
Wed Mar 19, 2003 6:36 am
Forum: Techniques and Tools
Topic: Bob Leatherbarrow's Class
Replies: 20
Views: 48539

I will be taking parts 2 and 3 of Bob's classes. Hope to meet a lot of folks and put faces and names together.