Re: Molds are there better Molds?

I'm from Colour de Verre and our molds were being discussed earlier in the thread. We only recommend two methods for priming our molds: MR-97 Aerosol Boron Nitride and Hotline Primo Primer. You can see videos about how to use the products at http://www.colourdeverre.com/go/primo and http://www.colou...