Search found 2 matches
- Tue Apr 22, 2003 10:16 pm
- Forum: Techniques and Tools
- Topic: BIG bubbles!
- Replies: 15
- Views: 25012
I have a Paragon kiln using a 12x8 kiln shelf. I checked the level of the kiln, and it's perfectly flat. No variations at all (nice to know I can rule that out). :) I'm making my own cabochons that I use in jewelry making, as well as some pendants. Usually I start with larger pieces, around 1 to 1 1...
- Tue Apr 22, 2003 9:46 am
- Forum: Techniques and Tools
- Topic: BIG bubbles!
- Replies: 15
- Views: 25012
BIG bubbles!
I know this has been discussed before. I'm just starting out, and I've been using this forum as a guide to any problems I've had. I had problems with small bubbles right at first and then looked it up here. Found out I needed to slow down the ramp to temperature. That really worked nice! However, al...