Search found 4 matches
- Fri Oct 14, 2016 6:52 pm
- Forum: Techniques and Tools
- Topic: Mystery contamination discolors piece
- Replies: 4
- Views: 8252
Re: Mystery contamination discolors piece
One heartening thing is that most of the red stuff is coming off with the sandpaper. Not sure I can get it out of the deepest areas. Does look like whatever is was fumed from a point in the center of the piece - can see radial streaks clearly as it is sanded off. I noticed the lid to my kiln wash ja...
- Fri Oct 14, 2016 3:56 pm
- Forum: Techniques and Tools
- Topic: Mystery contamination discolors piece
- Replies: 4
- Views: 8252
Re: Mystery contamination discolors piece
Thanks, Barry! I do know about the potential for silver contamination, and I was worried about that when I started planning this piece (which was why I used the cheapo piece of tile for a shelf). But in this case I don't think it was the silver - or if it was, it was something pretty indirect in whi...
- Fri Oct 14, 2016 2:42 pm
- Forum: Techniques and Tools
- Topic: Mystery contamination discolors piece
- Replies: 4
- Views: 8252
Mystery contamination discolors piece
During a tack fuse of my piece I was firing on thinfire laid on a kilnwashed ceramic tile (used many times before, but not for some time now). I suspect there was something on the tile because underneath the middle of the piece the thinfire turned gray. There is a difference in the surface of the gl...
- Mon Dec 17, 2007 2:04 pm
- Forum: Techniques and Tools
- Topic: leaf inclusions
- Replies: 0
- Views: 8610
leaf inclusions
I have been playing with leaves as inclusions and have the same problem I have seen in the archives - bubbles around the leaves. The galling thing is that it worked well once and then not when I repeated it - perhaps I should just take my gift from the kiln gods and stop. Based on what I saw in the ...