Views: 14106

I started warm glass about 1 month ago. I started with a S96 glass pack and noticed that one of the pieces had a spectrum waterglass sticker under the S96 sticker. This got me thinking about the rest of my regular spectrum glass, so I tested all my spectrum glass against spectrum 96 clear.About 85% ...