Re: How can we make dichroic nametags?
Thank you for all the suggestions! This forum is really fantastic! Just wanted to let you know that since I had some stickers, I did try them and it did work! Thank you Julie! I even reversed it by putting the stickers on, using a sharpie marker to paint out the background, peeled the stickers off a...