Float Glass is cracking

Hi All, I'm trying to make pocket vases using float glass. 1/8 inch on the bottom layer and 1/4 on the top. They measure 6x12 with a 1/2 inch fiber blanket in between to form the pocket. I've used 14 guage copper wire to use as hangers. My firing cycle is as follows. 250dph to 750. Hold 10 min. 9999...