Search found 8 matches

by Nancy D
Thu Feb 19, 2004 11:44 pm
Forum: Techniques and Tools
Topic: FLORIDA ANYONE?
Replies: 23
Views: 44504

Re: Florida Anyone?

<<Art Glass house is in Cocco>>

Make that Cocoa. :o)
by Nancy D
Thu Dec 11, 2003 8:42 pm
Forum: Techniques and Tools
Topic: Glass Getaway 2004 in Palm Beach?
Replies: 3
Views: 7433

Thanks Bobbie and Vernelle.
That's what I needed to know. I'd really like to go.
I appreciate your help.
bye Nancy
by Nancy D
Mon Dec 08, 2003 11:48 pm
Forum: Techniques and Tools
Topic: Glass Getaway 2004 in Palm Beach?
Replies: 3
Views: 7433

Glass Getaway 2004 in Palm Beach?

Hello, Does anyone one know anything about the Glass Getaway in Palm Beach, FL. It's to be held in February and sponsered by The Glass Craftsman Magazine. I'm fairly new to working with glass and would love to learn more about painting with frits and enamels. Any comments would be apprecitated. Than...
by Nancy D
Sun May 25, 2003 10:00 pm
Forum: Techniques and Tools
Topic: Broken slumped bottle lamp shade
Replies: 1
Views: 4730

I'm going to try to one more time to get the photo to show up again..

Image

I'm thinking the kiln went up too fast for the bottles which caused the splits.
Thanks, Nancy D.
by Nancy D
Fri May 23, 2003 10:42 pm
Forum: Techniques and Tools
Topic: Broken slumped bottle lamp shade
Replies: 1
Views: 4730

Broken slumped bottle lamp shade

A fused, then slumped lamp shade made of the small perrier bottles came out of the kiln today split on opposing bottles. Here is the firing schedule; 225dph to 600o-no hold, 300dph to 1200-held for 15 minutes. The kiln was supposed to go up to 1325 and hold there some, but when I looked at the piece...
by Nancy D
Tue Mar 18, 2003 9:00 pm
Forum: Techniques and Tools
Topic: Gerry's Casting Mix ?
Replies: 6
Views: 15925

Jack,
Thanks so much for the web sites! The second is a great help.
bye Nancy
by Nancy D
Fri Mar 14, 2003 10:37 pm
Forum: Techniques and Tools
Topic: Gerry's Casting Mix ?
Replies: 6
Views: 15925

Thanks, Becky, that's what I needed to know.
bye Nancy D.
by Nancy D
Fri Mar 14, 2003 5:24 pm
Forum: Techniques and Tools
Topic: Gerry's Casting Mix ?
Replies: 6
Views: 15925

Gerry's Casting Mix ?

Hello, I have some Gerry's Casting Mix that came with no instructions (I've asked the supplier for the information but haven't heard back from them). The archives here ( I love this board!!) gave some help, but I still have one more question. Do the molds made with this mix need to have a kiln wash ...