Search found 2 matches

by Jennifer
Thu May 08, 2003 3:12 pm
Forum: Techniques and Tools
Topic: Demonic Posession?
Replies: 9
Views: 14131

Thanks Tony! You were right, the relay is broken. I called the manufacturer and they are sending a new one as it is still under warrenty.

I too, am wondering if this is such a common problem then why don't they install the overide as a standard on all kilns.
Thanks to everyone for their input.
by Jennifer
Thu May 08, 2003 1:15 am
Forum: Techniques and Tools
Topic: Demonic Posession?
Replies: 9
Views: 14131

Demonic Posession?

Previously a glass blowing apprentice, I have been fusing for a short time. Up until this point I have had only small problems that I 've been able to figure out until tonight. I went to my studio and turned on the kiln to fuse two small plates. Schedule: 400 dph to 1250 200 dph to 1350 ( I was fire...