Search found 1 match

by Lodahl Art Glass
Thu Jan 17, 2008 5:26 pm
Forum: Techniques and Tools
Topic: Help with Black Cupric Oxide?
Replies: 0
Views: 9433

Re: Help with Black Cupric Oxide?

thank you Rosanna. Could you tell me how high you fired it? I fired 4 tiles and was real careful about not putting any tin sides against the oxide. Maybe the firing schedule I used wasn't enough heat?