Robin, Another easy way to get bettter adherence is to use a bit of clear powder between the design element and the irid surface. Just coat the back of the design element with a bit of GlasTac (or something similar) and dip it into clear powder. Then place it, powder side down, on the irid surface ...
- Sun Jan 18, 2004 9:20 am
- Forum: Kiln Casting
- Topic: glass fusion in a sterling silver finding
- Replies: 15
- Views: 32067
Re: glass fusion in a sterling silver finding
I know you can use PMC to create a bezel around glass or another lapidary material then fire at a low temp to create a finding. I wanted to know if someone could buy a sterling silver bezel cup from a company like Rio Grande- put your glass into the cup then do a full fusion. I was thinking the shr...
- Sun Dec 07, 2003 8:59 am
- Forum: Techniques and Tools
- Topic: Searching for button findings...
- Replies: 13
- Views: 32937
Andrew wrote: Try http://www.dymax.com. When dymax works, it is a solid bond. It can be tricky to use. The accelerator needs to be applied in a very thin coat and then allowed to dry. Then light clamping (I use clothes pins) for a couple of hours. AJW Dee Wrote: interesting, when i use it to adhere...
- Mon Oct 20, 2003 1:29 am
- Forum: Techniques and Tools
- Topic: Good art quotes
- Replies: 23
- Views: 40378
- Sun Aug 03, 2003 9:37 am
- Forum: Techniques and Tools
- Topic: fired a cab, top layer of glass did not flat fuse
- Replies: 14
- Views: 23016
- Sun Aug 03, 2003 9:32 am
- Forum: Techniques and Tools
- Topic: fired a cab, top layer of glass did not flat fuse
- Replies: 14
- Views: 23016
- Thu Jun 12, 2003 9:58 am
- Forum: Kiln Casting
- Topic: Help, need pyrometer/controller - electritian
- Replies: 3
- Views: 9056
Good Morning, I'm over 15(way over) but will try to help. Sometimes sellers on EBAY(or any retail store for that matter) don't know much about what they are selling, it would be nice if they would admit it. Oh well. Controllers can be very confusing, I have some experience, maybe we can muddle throu...