Search found 592 matches

by Buttercup
Tue Sep 23, 2025 1:04 am
Forum: Kiln Casting
Topic: Casting Reichenbach?
Replies: 3
Views: 212446

Re: Casting Reichenbach?

Er, Kris....Amanda's post was eleven years ago, but I'm sure someone will benefit from your post, too. :D
by Buttercup
Fri Sep 05, 2025 3:32 am
Forum: Techniques and Tools
Topic: Dealing with bubble in glass
Replies: 13
Views: 206901

Re: Dealing with bubble in glass

You've received lots of excellent advice. One possibility for bubble formation I didn't see mentioned yet is that the holes in the bottom of the mold may not be clear of kiln wash or other debris, and if they are clear, that the mold may not have been slightly elevated above the kiln shelf so the ho...
by Buttercup
Sat Aug 23, 2025 12:23 am
Forum: Newcomer Forum
Topic: Evaluating a used kiln
Replies: 1
Views: 46469

Re: Evaluating a used kiln

Hi Doug, welcome to the board. You don't say, but do you have any experience with kilns? I can't advise about Evenheat as I've never owned that brand but a search in the search field using the information about that make and the model number might bring up some posts or threads with useful informati...
by Buttercup
Sat Aug 02, 2025 10:17 pm
Forum: Techniques and Tools
Topic: Using raw oxides to color glass
Replies: 4
Views: 98129

Re: Using raw oxides to color glass

Hi Chelsea,
This board is a great resource, isn't it?

Have you experimented with any of the suggestions yet? Ready to post any pictures?
by Buttercup
Mon May 12, 2025 4:08 am
Forum: Techniques and Tools
Topic: controller for small Aims kiln
Replies: 11
Views: 212140

Re: controller for small Aims kiln

Hi Bonnie,
I have had a DIGITRY GB4 controller that will run five kilns for thirty plus years. I've never used that many kilns but search this board and you'll probably find lots of references to them. I like it very much.
by Buttercup
Sun Apr 20, 2025 9:21 pm
Forum: Kiln Casting
Topic: Kiln dust falls from lid
Replies: 1
Views: 895266

Re: Kiln dust falls from lid

Hi Kilninit, Welcome to the WGB. If you want help on a particular topic or piece of equipment you will be more likely to get a useful answer if you include specifics. In this case the type of kiln you are using, make and model or, if homemade, a description of how it is made: fire brick with a fibre...
by Buttercup
Wed Mar 19, 2025 7:44 am
Forum: Techniques and Tools
Topic: Film and Halos around painted lines
Replies: 14
Views: 253691

Re: Film and Halos around painted lines

Maybe the contamination has burned off now?

There's a proper scientific term for that, I'm sure, but it's late.
by Buttercup
Sun Jan 12, 2025 3:45 am
Forum: Techniques and Tools
Topic: powdered frit "paper"?
Replies: 3
Views: 94865

Re: powdered frit "paper"?

Can you remember if you had a kiln when you made it?

If so, could it be a powder wafer?
by Buttercup
Sat Dec 28, 2024 6:05 pm
Forum: Kiln Casting
Topic: Tempered glass shards
Replies: 1
Views: 117393

Re: Tempered glass shards

Hi, and welcome to the board. Type 'Morganica tempered glass' into the search bar. If that doesn't get you enough posts to answer your question try just typing 'Fusing tempered glass'. I do remember several years ago that Morganica posted quite a bit about her experiments with tempered shards. You a...
by Buttercup
Tue Nov 19, 2024 3:41 am
Forum: Techniques and Tools
Topic: Film and Halos around painted lines
Replies: 14
Views: 253691

Re: Film and Halos around painted lines

Just came across this older thread where one of the contributors mentions a film on the glass. I don't know if it's the same problem as yours but the answers that follow may help you:

viewtopic.php?p=363859&sid=5b17e9dc7625 ... e0#p363859
by Buttercup
Sun Nov 10, 2024 7:15 pm
Forum: Techniques and Tools
Topic: Film and Halos around painted lines
Replies: 14
Views: 253691

Re: Film and Halos around painted lines

I won't wade into the 'halo' discussion as I've not experienced it.I'd like to make a suggestion about your house wiring in preparation for a kiln. Disclaimer: I am not an electrician. This is about my personal experience. Unless your house is really old with dodgy wiring that should be replaced any...
by Buttercup
Sun Mar 10, 2024 2:51 am
Forum: Techniques and Tools
Topic: Glass carving gun (abrasive blasting)
Replies: 5
Views: 67934

Re: Glass carving gun (abrasive blasting)

Thank you so much, Brad! I'll see if I can make contact. :D Bingo! After much searching with no luck I found another site that seems to be related and shows long-lasting tips. I haven't made actual contact yet as it's the weekend but I'll contact the vendor and report back in case it helps someone ...
by Buttercup
Sun Mar 10, 2024 1:46 am
Forum: Techniques and Tools
Topic: Glass carving gun (abrasive blasting)
Replies: 5
Views: 67934

Re: Glass carving gun (abrasive blasting)

Thank you for those suggestions, Kevin. It seems that Butch doesn't have her on-line store anymore. I checked the others, too. Although small tips (1/16" and 3/32") are available I couldn't find any info about the gun they were made for, Empire. There are local suppliers with small ceramic...
by Buttercup
Thu Mar 07, 2024 4:40 am
Forum: Techniques and Tools
Topic: Large Kiln Shelves, redux
Replies: 11
Views: 84150

Re: Large Kiln Shelves, redux

Hi Buttercup! Unfortunately, my local supplier only stocks the Unifrax HD boards in 24" x 36". To special order a larger board was ridiculously expensive and I'd be stuck with massive quantities of HD board! #-o P.S. You didn't mention your winning lottery ticket numbers! I'm all ears! Tr...
by Buttercup
Wed Mar 06, 2024 8:04 pm
Forum: Techniques and Tools
Topic: Glass carving gun (abrasive blasting)
Replies: 5
Views: 67934

Re: Glass carving gun (abrasive blasting)

Thank you so much, Brad! I'll see if I can make contact. :D
by Buttercup
Wed Mar 06, 2024 8:31 am
Forum: Techniques and Tools
Topic: Large Kiln Shelves, redux
Replies: 11
Views: 84150

Re: Large Kiln Shelves, redux

How do you plan to lift it? 8-[

Edit: Oops, missed the 'light-as-a-feather' reference!

I like the HD fibre board. Do they come big enough for your project?
by Buttercup
Tue Mar 05, 2024 1:26 am
Forum: Techniques and Tools
Topic: Glass carving gun (abrasive blasting)
Replies: 5
Views: 67934

Glass carving gun (abrasive blasting)

I'm hoping someone can help me out with a brand name and specs. for a good sand carving gun. The excellent one I had in Canada didn't make it here. Possibly Border Security thought it was a weapon and we have really strict rules about those. Or maybe it just got nicked, anyway, I don't have it and w...
by Buttercup
Mon Feb 26, 2024 8:13 pm
Forum: Techniques and Tools
Topic: Red Devil DP2 Diamond points
Replies: 3
Views: 55327

Re: Red Devil DP2 Diamond points

Hi, Don!
by Buttercup
Fri Feb 23, 2024 2:53 am
Forum: Techniques and Tools
Topic: Red Devil DP2 Diamond points
Replies: 3
Views: 55327

Re: Red Devil DP2 Diamond points

I have received confirmation from Fletcher-Terry that their #2 1/2 Diamond points will fit the DP 2 Point driver.
by Buttercup
Tue Feb 20, 2024 11:54 pm
Forum: Techniques and Tools
Topic: Red Devil DP2 Diamond points
Replies: 3
Views: 55327

Red Devil DP2 Diamond points

I have an elderly Red Devil DP 2 Point setter (no, not the red flower). It's a little hand-operated tool for firing diamond-shaped fasteners into window frames or picture frames to secure the glass in place.Great tool. I no longer have the box the points came in so don't know what size to order. The...