Search found 11 matches

by Richard Carder
Sun Aug 11, 2013 5:19 am
Forum: Techniques and Tools
Topic: Gluing Transparent coloured glass to white board?
Replies: 4
Views: 9256

Gluing Transparent coloured glass to white board?

Hi
I want to glue a glass painting to a white base board without the glue showing underneath the transparent glass, any ideas?
by Richard Carder
Thu Jul 25, 2013 7:33 am
Forum: Techniques and Tools
Topic: Dichro Question
Replies: 3
Views: 7193

Dichro Question

I am just about to fuse some dichro glass cufflinks. One problem I always find is that once fired there is a black surround of the dichro glass when I am using dichro with a black base. Can anyone suggest either through firing sched or other ideas that I can have only dichro glass showing?
by Richard Carder
Fri Mar 15, 2013 7:54 am
Forum: Techniques and Tools
Topic: Air Bubble in large panel when slumping.
Replies: 12
Views: 22028

Re: Air Bubble in large panel when slumping.

Just open kiln and my panel is perfect. Thanks everyone for advice.
by Richard Carder
Thu Mar 07, 2013 2:40 pm
Forum: Techniques and Tools
Topic: Air Bubble in large panel when slumping.
Replies: 12
Views: 22028

Re: Air Bubble in large panel when slumping.

Thanks everyone.
by Richard Carder
Thu Mar 07, 2013 12:05 pm
Forum: Techniques and Tools
Topic: Air Bubble in large panel when slumping.
Replies: 12
Views: 22028

Re: Air Bubble in large panel when slumping.

Oh yes, the thickness is 3mm with fused frit on top.
by Richard Carder
Thu Mar 07, 2013 12:04 pm
Forum: Techniques and Tools
Topic: Air Bubble in large panel when slumping.
Replies: 12
Views: 22028

Re: Air Bubble in large panel when slumping.

Hi, the firing schedual is in cent, 85,538,20,85,633,5,465,716,12,Full,488,60,20,445,10,215,150
by Richard Carder
Thu Mar 07, 2013 8:42 am
Forum: Techniques and Tools
Topic: Air Bubble in large panel when slumping.
Replies: 12
Views: 22028

Re: Air Bubble in large panel when slumping.

Yes, I have raised it off the kiln floor to let the air escape through the air holes.
by Richard Carder
Thu Mar 07, 2013 2:29 am
Forum: Techniques and Tools
Topic: Air Bubble in large panel when slumping.
Replies: 12
Views: 22028

Air Bubble in large panel when slumping.

Hi, when slumping a large panel 8" x 15" on a wave mould I always get a large air bubble in the middle of the piece. I have air holes in the mould. The only thing I can think that is causing it is that panel is slight thickness differences in the panel.
by Richard Carder
Sun Jan 20, 2013 1:10 pm
Forum: Techniques and Tools
Topic: Thermal Shock Cracking Whilst Slumping
Replies: 3
Views: 6744

Re: Thermal Shock Cracking Whilst Slumping

Thanks for your reply. The edge of the glass where it cracked is rounded, so it make me think that it cracked during heating up, so I will slow it down.
by Richard Carder
Sun Jan 20, 2013 11:58 am
Forum: Techniques and Tools
Topic: Thermal Shock Cracking Whilst Slumping
Replies: 3
Views: 6744

Thermal Shock Cracking Whilst Slumping

I have just slumped a dish 11" square. The total thickness of the dish is 6mm, Bullseye glass. The kiln that I am using is a Paragon Fusion 8. The firing schedule whilst annealing is 522c for 1 hour. When I opened the kiln there was a clean crack along the centre of the dish. There must be some...
by Richard Carder
Tue Aug 14, 2012 11:12 am
Forum: Techniques and Tools
Topic: Christmas Tree Decorations
Replies: 1
Views: 4993

Christmas Tree Decorations

I am preparing my stock for the Christmas Craft Markets and I would like some ideas on simple Christmas Tree decorations that I can sell, any ideas please. :)