Search found 114 matches
- Sat Nov 08, 2014 3:10 pm
- Forum: Newcomer Forum
- Topic: 4 Seasons.... Break
- Replies: 12
- Views: 16299
Re: 4 Seasons.... Break
@ @ Valerie Adams and Vonon: Thank you for your answer ! Yes, in any case I will try to repair this piece...... but I use somewhat help: 1) The first break was repaired the same day: A blank System96 (as the rest of the used glass) (partly.... so not the whole piece !) UV glued on the break. Questio...
- Thu Nov 06, 2014 9:18 am
- Forum: Newcomer Forum
- Topic: 4 Seasons.... Break
- Replies: 12
- Views: 16299
Re: 4 Seasons.... Break
@ Stephen Richard: Thank you for your answer. Yes, you are right..... no annealing. But.... I did not fire myself and very surprised that my relative used this programm ! But...... is there anyone please , who can give advise about my question to try to repair this piece ?? Gluing on "Trespa&qu...
- Tue Nov 04, 2014 9:21 am
- Forum: Newcomer Forum
- Topic: 4 Seasons.... Break
- Replies: 12
- Views: 16299
Re: 4 Seasons.... Break
Hello ! Thank you all for your answers ! Firing programm below. I did not personally fire, as my kiln is too little. A relative with a bigger kiln did fire (and he did make more glassworks for outside and attached them.....but always in parts... and not so big !) @ Valerie Adams: Yes, a hard lesson ...
- Mon Nov 03, 2014 7:45 am
- Forum: Newcomer Forum
- Topic: 4 Seasons.... Break
- Replies: 12
- Views: 16299
4 Seasons.... Break
Hello ! With the link below you can see this glass (the 4 Seasons) on the wall( Then... okay), the first- and second breaking of the glass. Assuming that the firing was OK, what can be the reason of breaking ? The first break was alreay after half an hour after attach on the wall, the 2nd the next d...
- Tue Aug 06, 2013 10:05 am
- Forum: Newcomer Forum
- Topic: CONTOUR fuse spectrum96 opal glass
- Replies: 16
- Views: 15865
Re: CONTOUR fuse spectrum96 opal glass
Brad: Yes, using powder is a good idea. I have to make ca. 150 leaves for a tree and I don't like the effect ! Now I have to test what is the best way and also important... the quickest way
- Tue Aug 06, 2013 8:34 am
- Forum: Newcomer Forum
- Topic: CONTOUR fuse spectrum96 opal glass
- Replies: 16
- Views: 15865
Re: CONTOUR fuse spectrum96 opal glass
Brad, Thank you for the explanation ! I now understand it is the glass (and not the firing). I was thinking about grinding the glass with a 45 degrees angle (as far as possible of course). What do you think about this ? Jan
- Tue Aug 06, 2013 7:58 am
- Forum: Newcomer Forum
- Topic: CONTOUR fuse spectrum96 opal glass
- Replies: 16
- Views: 15865
Re: CONTOUR fuse spectrum96 opal glass
No solutions till now. I wonder...is it possible it comes from grinding ?? If yes, how can I avoid this ?
- Tue Aug 06, 2013 5:00 am
- Forum: Techniques and Tools
- Topic: Using Photo Fusing Paper for the first time
- Replies: 9
- Views: 13284
Re: Using Photo Fusing Paper for the first time
Hello,
Make the image in mirror and put the iron oxide side on the glass !!! The result is better as normal !!
Jan de Jong
Make the image in mirror and put the iron oxide side on the glass !!! The result is better as normal !!
Jan de Jong
- Tue Aug 06, 2013 4:16 am
- Forum: Newcomer Forum
- Topic: CONTOUR fuse spectrum96 opal glass
- Replies: 16
- Views: 15865
Re: CONTOUR fuse spectrum96 opal glass
Thank you Brad. An easier way
Jan
Jan
- Mon Aug 05, 2013 2:57 pm
- Forum: Newcomer Forum
- Topic: CONTOUR fuse spectrum96 opal glass
- Replies: 16
- Views: 15865
Re: CONTOUR fuse spectrum96 opal glass
For the working link you need name and password . As Snapfish stops next month, I can give you this (and there are only 2 images of this problem, and Snapfish have no address etc of me) Username and password removed, as I could attached the image below. On which site is it possible to share images ?...
- Mon Aug 05, 2013 1:47 pm
- Forum: Newcomer Forum
- Topic: CONTOUR fuse spectrum96 opal glass
- Replies: 16
- Views: 15865
Re: CONTOUR fuse spectrum96 opal glass
If you look at the edges of the glass you will see that one side is darker than the other Sorry Steve, I don't see that differnce !? Here you can see it http://www3.snapfish.nl/snapfishnl/fe/l=nl_NL/p/Organizer/s_c=0/s_mvm=NAP/s_ev20=NL_Google_2007/s_ru=FALSE/s_se=FDR/s_reg=1/s_cmpg=NL_Google_2007#...
- Mon Aug 05, 2013 8:24 am
- Forum: Newcomer Forum
- Topic: CONTOUR fuse spectrum96 opal glass
- Replies: 16
- Views: 15865
Re: CONTOUR fuse spectrum96 opal glass
oeps .. I mean the Chestnut DARker on the edges
- Mon Aug 05, 2013 4:59 am
- Forum: Newcomer Forum
- Topic: CONTOUR fuse spectrum96 opal glass
- Replies: 16
- Views: 15865
CONTOUR fuse spectrum96 opal glass
Hello!
I have troubles with this contour fuse: the edges of Dark Green (220-76) becomes lighter green and Chestnut (211-74 gets lighter edges.
I have no idea why ? And... is there something to do, to get it the right colour ?
Thank you for your help, Jan
I have troubles with this contour fuse: the edges of Dark Green (220-76) becomes lighter green and Chestnut (211-74 gets lighter edges.
I have no idea why ? And... is there something to do, to get it the right colour ?
Thank you for your help, Jan
- Mon Apr 05, 2004 3:50 pm
- Forum: Techniques and Tools
- Topic: Armstrong glass, possible or not ?
- Replies: 1
- Views: 3304
Armstrong glass, possible or not ?
Hello, a week ago I did slump glass destined for Stained glass(producer unknown - transparant with some orange) with good result. Got courage with this result and I could buy (cheap) 2 plates of Armstrong, with colours I did like. Did fuse the plate with white and blue (2 layers), and for your infor...
- Mon Mar 15, 2004 10:13 am
- Forum: Techniques and Tools
- Topic: Floatglass Break Help
- Replies: 7
- Views: 7947
Float crack
Just cut your glass so that it is the same diameter as the mold and can slide down in the inside a little. It would be good to know your firing schedule when answering questions like this. ch Charlie, thank you ! I did place more floatglass and slump and now I can use the mold for making a mold of ...
- Sat Mar 13, 2004 2:02 pm
- Forum: Techniques and Tools
- Topic: Floatglass Break Help
- Replies: 7
- Views: 7947
Float Mold Crack
Bert, Soft edges.. so heatup crack, you think. It is not possible that the amount of glass was too low????? It had no possibilty to flow enough ? Or what will happen then ? Just want to know for projects in the future! Yes, for a better mold I have to use plaster + silica, but this contra-mold was j...
- Sat Mar 13, 2004 10:42 am
- Forum: Techniques and Tools
- Topic: Floatglass Break Help
- Replies: 7
- Views: 7947
Floatglass Break Help
Hi all! Did make a contra-mold from (only) plaster in order to make a mold. And from the made-mold I wish to make a ceramic mold (for more firings) I lay 1 piece of Float on the plaster mold and just open the kiln: The glass has in the middle a crack. (see the image, link below) Due to.................
- Sat Mar 06, 2004 11:41 am
- Forum: Photos and Stuff
- Topic: Had to try Potmelt
- Replies: 8
- Views: 9996
Had to try a potmelt
Hi!
I like your potmelts! Great! Have to try it myself soon.
A question: what is the diameter of these potmelts and the thickness ?
Oh, and the diameter of the flowerpot?
Jan
I like your potmelts! Great! Have to try it myself soon.
A question: what is the diameter of these potmelts and the thickness ?
Oh, and the diameter of the flowerpot?
Jan
- Fri Jan 30, 2004 11:57 am
- Forum: Techniques and Tools
- Topic: Lambert's glass
- Replies: 4
- Views: 6010
Lambert's Glass
Hello,
No, but perhaps you can find something here:
http://www.lamberts.de/elambhom.htm[img]
Jan[/img]
No, but perhaps you can find something here:
http://www.lamberts.de/elambhom.htm[img]
Jan[/img]
- Wed Jan 21, 2004 2:02 pm
- Forum: Techniques and Tools
- Topic: Light bulb
- Replies: 0
- Views: 7093
Light bulb