Search found 31 matches
- Sun Aug 31, 2003 1:38 am
- Forum: Techniques and Tools
- Topic: slump failure help?
- Replies: 2
- Views: 5221
slump failure help?
Just slumped my first large 17 inch deep BE bowl. The first fuse came out gr8....beautiful red transparent with stringers etc....then I put it into a mold to slump.....bowl shrunk down from original diamenter of 17 in to 14 and got one big bubble in the center. Didnt pop and kinda looks interesting ...
- Tue Aug 26, 2003 2:48 pm
- Forum: Techniques and Tools
- Topic: keeping holes in glass
- Replies: 6
- Views: 7731
HOLES
The bottom is clear glass without holes........top is red which I so carefully and tediously drilled about 10 holes 1/4" diameter.........want to keep them from closing for light reflecting thru and for polka dotted affect. Thanks for all your input.......could I also just cut same size out of ...
- Tue Aug 26, 2003 12:48 pm
- Forum: Techniques and Tools
- Topic: keeping holes in glass
- Replies: 6
- Views: 7731
keeping holes in glass
I have drilled holes in a large red transparent glass...wanting a polka-dotted effect........bottom layer is clear. Questions...1) Will the holes close up when I fuse it and if so, how can I keep that from happening? 2) This will be slumped as a deep bowl and I would like some design to show on the...
- Sun Aug 24, 2003 12:02 pm
- Forum: Photos and Stuff
- Topic: please comment
- Replies: 5
- Views: 7986
comments?????????????
This site is now accessible......Really hoping for some feedback from all you professional fusers
- Sat Aug 23, 2003 11:59 am
- Forum: Photos and Stuff
- Topic: please comment
- Replies: 5
- Views: 7986
uploading?
how to we post pics from shutterfly??
- Sat Aug 23, 2003 1:56 am
- Forum: Photos and Stuff
- Topic: please comment
- Replies: 5
- Views: 7986
please comment
ok, think i figured it out...would you please comment on my very first time firing.. much thanks.. rj
- Thu Aug 21, 2003 1:54 am
- Forum: Techniques and Tools
- Topic: Looking for Special Slumping mold and need help
- Replies: 6
- Views: 6628
- Thu Aug 21, 2003 1:29 am
- Forum: Techniques and Tools
- Topic: bubbles galore
- Replies: 3
- Views: 4708
thanks
i think my kiln is firing 'hot'
- Wed Aug 20, 2003 9:32 am
- Forum: Techniques and Tools
- Topic: Firing Schedules for glass book
- Replies: 1
- Views: 2843
book
Yes, just got one.....Artisan Books......I spoke with Penelope Johns in Australia...Phone (03)94164805 Fax (03)94164806 http://www.artisan.com.au...cost about $100 plus shipping......takes around 2 wks......
- Wed Aug 20, 2003 9:27 am
- Forum: Techniques and Tools
- Topic: bubbles galore
- Replies: 3
- Views: 4708
bubbles galore
:roll:Help the newbies........we need it :cry: Made my first piece - 15 inch round , clear bottom-black top plus design....fired 300 yada yada up to 1420..wanted tack fuse..got..........bubbles....and full fuse...no thin fire paper......ok next one...used fire paper........large round 17 inch 2 lay...
- Wed Aug 20, 2003 12:38 am
- Forum: Techniques and Tools
- Topic: help..what to do with kosta boda
- Replies: 14
- Views: 13079
kosta boda
I know it can never be wha it was. What I had in mind was to just lay all the pieces on the bottom of the shelf and fuse it toone flat piece and then go from there. Question? can I fuse crystal.....not with anything strange with it.....will it ;blow up and ruin my kiln? just fuse the pieces like you...
- Mon Aug 18, 2003 10:42 pm
- Forum: Techniques and Tools
- Topic: help..what to do with kosta boda
- Replies: 14
- Views: 13079
kosta boda
crystal from sweden
- Mon Aug 18, 2003 10:33 pm
- Forum: Techniques and Tools
- Topic: help..what to do with kosta boda
- Replies: 14
- Views: 13079
help..what to do with kosta boda
kids broke a very expensive kosta boda baloon-shaped piece.....now I have a box of gorgeous pieces of rainbow colored crystal..........can i fuse it ? If so, on shelf ? do i need to contain it in some way?
- Mon Aug 18, 2003 10:27 pm
- Forum: Techniques and Tools
- Topic: glass cleaner panic
- Replies: 20
- Views: 21997
try this
I mix 1/3 rubbing alcohol, 1/2 water, 1/3 ammonia (no suds)......in a spray plastic bottle.............works gr8
- Sat Aug 16, 2003 11:18 am
- Forum: Techniques and Tools
- Topic: pattern bars
- Replies: 12
- Views: 11671
pattern bars
would appreciate help for first time pattern bar maker. .........want to make long strips and stack.........about 7 layers high.....how do I set up and what is a GOOD firing schedule (24 jen-ken) yes, already checked archives...........no firing schedule
- Thu Aug 14, 2003 11:00 pm
- Forum: Techniques and Tools
- Topic: prepping up a new kiln
- Replies: 9
- Views: 9872
215 blade
what brand is that and will it fit onto any 7 inch saw?
- Thu Aug 14, 2003 10:38 pm
- Forum: Techniques and Tools
- Topic: prepping up a new kiln
- Replies: 9
- Views: 9872
kiln wash
I used Bullseye Kiln Wash and the kiln is Jen-Ken 24 including shelf..This is the tile saw I bought .brank is American Forge....They did seem to know what blade to suggest for glass........They thought I was nuts for cuttin glass like that :lol: . This is the 7" heavy duty wet tile saw. This sa...
- Thu Aug 14, 2003 10:08 pm
- Forum: Techniques and Tools
- Topic: prepping up a new kiln
- Replies: 9
- Views: 9872
prepping up a new kiln
Just got my new kiln and very anxious to get firing sooooo. cleaned bottom of kiln from all dust, applied was as suggested to bottom and prepared the shelf.....smoothing it and then applying kiln....rather than waiting a few days, I heated the kiln to 500...venting every s often...so that I wouldnt ...
- Tue Aug 12, 2003 9:03 pm
- Forum: Techniques and Tools
- Topic: compresor for axtec
- Replies: 7
- Views: 7736
air compressor
:lol: Avery, thanks for your help. I am sure the compressor you mentioned will be just fine. I am a newbie at all this (just got my kiln today) and dont even know how to airbrush but I got caught up in the 'shopping madness for aztec'. ....hope Ill be as successful in my firing..BTW, the girl at Mic...
- Mon Aug 11, 2003 3:34 pm
- Forum: Techniques and Tools
- Topic: compresor for axtec
- Replies: 7
- Views: 7736
compresor for axtec
ok got lucky and got my Michaels 'deal'..........now what compressor should I buy?