Search found 3 matches

by Marz
Tue Jun 19, 2012 9:35 am
Forum: Newcomer Forum
Topic: Drilling holes in Molds
Replies: 8
Views: 22684

Re: Drilling holes in Molds

The copper is .004" thick. There is only one hole in the center of the mold.
by Marz
Mon Jun 18, 2012 11:40 pm
Forum: Newcomer Forum
Topic: Drilling holes in Molds
Replies: 8
Views: 22684

Re: Drilling holes in Molds

Brad, Thanks for your thoughts. I know that the air hole wasn't blocked because just before it was fired someone noted that the hole was plugged and we fixed that. I don't have the firing schedule since these were done at a local glass school. (long story) I've included a couple of pics (at least I ...
by Marz
Mon Jun 18, 2012 4:27 pm
Forum: Newcomer Forum
Topic: Drilling holes in Molds
Replies: 8
Views: 22684

Drilling holes in Molds

So, I slumped into a new circular plate mold for the first time and ended up with what looks like voids on the bottom. Someone suggested that what might have happened is that the middle of the glass slumped first, and blocked off the air hole, the edges sealed and the remaining air got pushed to the...