Re: using embedded fused glass in cement countertop

Hi Kim
I have just finished casting and staining a cement table top with a 12 x 12 fused glass textured greenman tile inset into the cement.

I used the reversed process of casting this (table top was on the bottom of the form. The tile appears to be very well set in the cement.

HTH,
Seth