Hi!
Has anyone here successfully cast bi-convex shapes (like lenses or domed pieces with curvature on both sides)? Any tips would be helpful…thanks!
Search found 5 matches
- Sat Jan 31, 2026 9:13 am
- Forum: Kiln Casting
- Topic: Bi-convex shapes
- Replies: 0
- Views: 114906
- Fri Sep 05, 2025 5:52 am
- Forum: Kiln Casting
- Topic: COE 104...
- Replies: 0
- Views: 180524
COE 104...
Hi!
I plan to cast some COE 104 Moretti glass. Does anyone have experience working with this glass? I’m particularly interested in the recommended firing schedule... I intend to make a glass hemisphere with a diameter of about 3.5 inches...
Thanks!
I plan to cast some COE 104 Moretti glass. Does anyone have experience working with this glass? I’m particularly interested in the recommended firing schedule... I intend to make a glass hemisphere with a diameter of about 3.5 inches...
Thanks!
- Mon Dec 10, 2012 6:33 pm
- Forum: Techniques and Tools
- Topic: Thin glass slumping
- Replies: 4
- Views: 8206
Re: Thin glass slumping
It's a gentle bend. I'm plating an old painted piece of glass with multiple (bonded) cracks. It's some kind of reinforcement of the back. The original it's bended to ( helical twist)
- Sun Dec 09, 2012 1:44 pm
- Forum: Techniques and Tools
- Topic: Thin glass slumping
- Replies: 4
- Views: 8206
Re: Thin glass slumping
Thanks for help. I need this glass for plating- so adding texture it's a problem...any advise about the mold?
- Fri Dec 07, 2012 6:22 am
- Forum: Techniques and Tools
- Topic: Thin glass slumping
- Replies: 4
- Views: 8206
Thin glass slumping
Hello everybody,
I need some help about mold making/firing schedule for slumping thin (1mm)glass. I must warp a little a 8x8" piece of clear float glass (I must take the shape from another -original- glass)
Thanks
I need some help about mold making/firing schedule for slumping thin (1mm)glass. I must warp a little a 8x8" piece of clear float glass (I must take the shape from another -original- glass)
Thanks