Re: Workbench top
Good idea - first I think I'll ask Charlotte why she wants to mark on it!
- Mon Jul 01, 2013 5:54 pm
- Forum: Techniques and Tools
- Topic: Workbench top
- Replies: 6
- Views: 12964
Re: Workbench top
Thanks Charlie. I mark on the strip cutter often, and am not sure why I'd want to mark on the tabletop, but my daughter, who shares the equipment, asked about this.
Lynn
Lynn
- Mon Jul 01, 2013 4:58 pm
- Forum: Techniques and Tools
- Topic: Workbench top
- Replies: 6
- Views: 12964
Workbench top
My strip cutter is on a melamine board, and I'm able to use a Sharpie on it, then clean it off with alcohol. Can you do the same thing with a matte Formica? I'm having a workbench built, and haven't decided what to use for the top. The melamine I've seen is glued to what seems to be a pretty crumbly...