Thank you Paul for your sample firing schedule. I am sure I will get much better results from my next firing.
As advised I will do some tests with slumping and will be very careful with the annealing of the "wedding stuff"!
Kind regards
Nikki
Search found 3 matches
- Fri Jun 20, 2003 7:23 am
- Forum: Techniques and Tools
- Topic: Float glass firing
- Replies: 4
- Views: 12031
- Thu Jun 19, 2003 10:04 am
- Forum: Techniques and Tools
- Topic: Float glass firing
- Replies: 4
- Views: 12031
- Thu Jun 19, 2003 8:29 am
- Forum: Techniques and Tools
- Topic: Float glass firing
- Replies: 4
- Views: 12031
Float glass firing
I have just opened my own Studio making stained glass but want to be able to make beautiful kiln fired glass pieces too. I was hoping someone could help me with some problems/questions about slumping float glass. I have a top loading flat bed kiln and so far I have tried fusing small pieces of float...