Search found 2 matches

by David Cutler
Wed Jun 25, 2003 9:39 pm
Forum: Techniques and Tools
Topic: Blasting Resist in a Pinch?
Replies: 8
Views: 16595

Maybe you should look at sign supply houses for the resist if there is one near you. The one I use stocks it regularly. Also you might try sign makers that specialize in wood sandcarved signs or monument makers in your town. They may sell you what you need if it is not much until your resist comes in.
by David Cutler
Wed Jun 18, 2003 12:44 am
Forum: Kiln Casting
Topic: Cutting cast slabs straight
Replies: 2
Views: 7434

I would suggest going to a custom granite countertop place. They usually have a large table with a saw that travels across it that could possibly do the job for you. You may want to check the width of there blade to see how much you are going to loose in material but this may be the easiest and quic...