Re: Hydrogen Sulfide from kiln wash

I looked up sulfur content of bamboo and it can be pretty high, so that appears to be the source of the sulfur, with the microbiological experiment inside the closed bucket being the cause. No more haik brushes left in the bucket for me! Happy Thanksgiving glass people!
by beaconglass
Sat Nov 23, 2013 10:07 am
Forum: Techniques and Tools
Topic: Hydrogen Sulfide from kiln wash
Replies: 11
Views: 20861

Hydrogen Sulfide from kiln wash

I had mixed some kilnwash a couple of months ago, and rather than rinsing the haik brush out, I left it in the kiln wash in a closed, plastic container (an old kiln wash cup). When I went to use it recently, I was almost overcome by hydrogen sulfide gas (rotten egg smell). The haik brush was covered...
by beaconglass
Thu Jan 24, 2013 3:50 pm
Forum: Techniques and Tools
Topic: Follow in devit question! Help with program please
Replies: 8
Views: 28847

Re: Follow in devit question! Help with program please

I'm no fusing expert, that's for sure, but it looks like your first program is un-necessarily slow heating from 1250 to 1480 (since you can't thermal shock the glass in that temp range), and it looks like your long hold at 1250 may also be contributing to de-vit, although I always thought de-vit onl...
by beaconglass
Wed Oct 03, 2012 1:10 pm
Forum: Techniques and Tools
Topic: BE kiln wash sticking to glass
Replies: 16
Views: 36902

Re: BE kiln wash sticking to glass

Is it possible your kiln temperature control is losing reliability? (running hotter than you think)
by beaconglass
Mon Oct 01, 2012 6:52 pm
Forum: Business Topics
Topic: Current Price of Silver and gold
Replies: 10
Views: 32718

Re: Current Price of Silver and gold

Wasn't $6/ounce silver nice! (I remember buying it at ~$3.50/oz not long before these 2004 posts, and now it's at what, $30/oz?)