Search found 6 matches
- Sun Sep 23, 2012 10:06 am
- Forum: Newcomer Forum
- Topic: Which molds?
- Replies: 15
- Views: 19064
Re: Which molds?
I am new to using molds as well, and over the past year I have tried some from Slumpys, Delphi and Bullseye. More recently I bought some of Laurie's bottomless molds and these are now my favorites. I don't have to set them on kiln furniture, just flat on the kiln shelf. The bottoms are perfectly fla...
- Thu Aug 16, 2012 10:17 pm
- Forum: Techniques and Tools
- Topic: Question about kiln wash shelf life
- Replies: 20
- Views: 24702
Re: Question about kiln wash shelf life
I don't have any of those except the spray nozzle, and I will try that. It's a pretty strong one, but not the power of a pressure washer by far.
- Wed Aug 15, 2012 10:47 pm
- Forum: Techniques and Tools
- Topic: Question about kiln wash shelf life
- Replies: 20
- Views: 24702
Re: Question about kiln wash shelf life
With casting molds I clean and rewash each time. It's a pain to clean the little crevices though, does anyone have a clever way to make that task more efficient?
- Mon Aug 13, 2012 7:31 pm
- Forum: Techniques and Tools
- Topic: Question about kiln wash shelf life
- Replies: 20
- Views: 24702
Re: Question about kiln wash shelf life
Thank you both, that is going to save me a lot of work!
- Mon Aug 13, 2012 5:24 pm
- Forum: Techniques and Tools
- Topic: Question about kiln wash shelf life
- Replies: 20
- Views: 24702
Re: Question about kiln wash shelf life
Interesting! So a mold will not have the same problem as a shelf does, if you do not change the wash each time? I would LOVE not to have to redo the molds.
- Mon Aug 13, 2012 3:19 pm
- Forum: Techniques and Tools
- Topic: Question about kiln wash shelf life
- Replies: 20
- Views: 24702
Re: Question about kiln wash shelf life
I'm so glad I found this discussion, I thought I was losing it. I kept reading that Primo was so easy to wipe off but that has not been the case for me. I just came in from sanding my two shelves. So it sounds like I am apparently mixing up too much wash (when I shake it up to use the next time it g...