Charlie, the soak you refer to is on the slump fire?
Do you do this on the ramp up or on the ramp down?
Are you both saying that you slump at ~1225? Are you using bullseye?
Thanks, Stephie
Search found 49 matches
- Thu Apr 08, 2004 2:02 pm
- Forum: Techniques and Tools
- Topic: contact marks when slumping
- Replies: 5
- Views: 5364
- Fri Mar 12, 2004 5:01 pm
- Forum: Photos and Stuff
- Topic: New Sink just delivered
- Replies: 20
- Views: 28400
- Mon Mar 08, 2004 6:55 pm
- Forum: Photos and Stuff
- Topic: Sink pictures (only a few of them)
- Replies: 35
- Views: 42111
- Fri Mar 05, 2004 4:46 pm
- Forum: Techniques and Tools
- Topic: Slumping pasta bowl?
- Replies: 12
- Views: 10693
- Fri Mar 05, 2004 2:48 pm
- Forum: Techniques and Tools
- Topic: Slumping pasta bowl?
- Replies: 12
- Views: 10693
- Fri Feb 27, 2004 11:03 am
- Forum: Techniques and Tools
- Topic: Dragon Molds
- Replies: 17
- Views: 17915
- Thu Feb 26, 2004 11:51 am
- Forum: Techniques and Tools
- Topic: Dragon Molds
- Replies: 17
- Views: 17915
Dragon Molds
Has anyone tried these?
I am going to C&R Loo tomorrow, they have them for 40% off. They are still expensive, are they worth it?
Thanks, Stephie
I am going to C&R Loo tomorrow, they have them for 40% off. They are still expensive, are they worth it?
Thanks, Stephie
- Thu Feb 19, 2004 12:33 pm
- Forum: Techniques and Tools
- Topic: I'm in LOVE!!
- Replies: 27
- Views: 32787
- Mon Feb 09, 2004 2:09 pm
- Forum: Techniques and Tools
- Topic: large sink slump
- Replies: 6
- Views: 6788
- Wed Dec 10, 2003 8:24 pm
- Forum: Techniques and Tools
- Topic: slumping overhang
- Replies: 5
- Views: 6238
- Fri Dec 05, 2003 5:26 pm
- Forum: Techniques and Tools
- Topic: Need help in how to fire a regular kiln for fusing and slump
- Replies: 7
- Views: 7357
Hi Sande, I also use a ceramic kiln. You can get a pyrometer (sp?) and probe (thermocouple) for less then $100. I drilled a hole in my peep hole plug to put the probe through. This lets me monitor the temp in the kiln and adjust the infinite switch accordingly. I think you are going to have to monit...
- Thu Dec 04, 2003 6:15 pm
- Forum: Techniques and Tools
- Topic: Fire polish after slump?
- Replies: 11
- Views: 15171
- Thu Dec 04, 2003 5:02 pm
- Forum: Techniques and Tools
- Topic: SS Rings
- Replies: 7
- Views: 7245
- Thu Dec 04, 2003 11:42 am
- Forum: Techniques and Tools
- Topic: Pyrometers..plates...bubbles agrhhhh!
- Replies: 16
- Views: 15530
Here is another place to get thermo & pyrometers.
http://www.omega.com/
http://www.omega.com/
- Wed Dec 03, 2003 12:19 pm
- Forum: Techniques and Tools
- Topic: I've got blisters on me fingers
- Replies: 10
- Views: 10443
- Mon Dec 01, 2003 2:39 pm
- Forum: Business Topics
- Topic: Glass Eye 2000
- Replies: 4
- Views: 5815
- Fri Nov 14, 2003 4:15 pm
- Forum: Techniques and Tools
- Topic: sinkhole question
- Replies: 6
- Views: 6241
- Thu Nov 13, 2003 11:36 am
- Forum: Techniques and Tools
- Topic: Setting up a warm glass studio.....
- Replies: 40
- Views: 40370
- Wed Nov 12, 2003 1:16 pm
- Forum: Techniques and Tools
- Topic: Atten: Jewelry Pendant artist
- Replies: 17
- Views: 18775
- Wed Nov 12, 2003 12:35 pm
- Forum: Techniques and Tools
- Topic: Atten: Jewelry Pendant artist
- Replies: 17
- Views: 18775