Search found 49 matches

by Stephie
Thu Apr 08, 2004 2:02 pm
Forum: Techniques and Tools
Topic: contact marks when slumping
Replies: 5
Views: 9485

Charlie, the soak you refer to is on the slump fire?
Do you do this on the ramp up or on the ramp down?
Are you both saying that you slump at ~1225? Are you using bullseye?
Thanks, Stephie
by Stephie
Fri Mar 12, 2004 5:01 pm
Forum: Photos and Stuff
Topic: New Sink just delivered
Replies: 20
Views: 43988

That is WONDERFUL Phil! =D> You must have a great deal of patience.
by Stephie
Mon Mar 08, 2004 6:55 pm
Forum: Photos and Stuff
Topic: Sink pictures (only a few of them)
Replies: 35
Views: 66820

Patty, where do you get those rings?
by Stephie
Fri Mar 05, 2004 4:46 pm
Forum: Techniques and Tools
Topic: Slumping pasta bowl?
Replies: 12
Views: 18950

:lol: Thank goodness!
I'd agree with Charlie, slow down
by Stephie
Fri Mar 05, 2004 2:48 pm
Forum: Techniques and Tools
Topic: Slumping pasta bowl?
Replies: 12
Views: 18950

Carla, are you slumping an inch and a half piece of glass, or is the bowl 1.5" deep?
by Stephie
Fri Feb 27, 2004 11:03 am
Forum: Techniques and Tools
Topic: Dragon Molds
Replies: 17
Views: 32538

No, not Dragons :lol:
I guess Dragon is the Manufacturer.
Thanks for the laugh!
by Stephie
Thu Feb 26, 2004 11:51 am
Forum: Techniques and Tools
Topic: Dragon Molds
Replies: 17
Views: 32538

Dragon Molds

Has anyone tried these?
I am going to C&R Loo tomorrow, they have them for 40% off. They are still expensive, are they worth it?
Thanks, Stephie
by Stephie
Thu Feb 19, 2004 12:33 pm
Forum: Techniques and Tools
Topic: I'm in LOVE!!
Replies: 27
Views: 54776

Pictures, PICTURES :lol:
by Stephie
Mon Feb 09, 2004 2:09 pm
Forum: Techniques and Tools
Topic: large sink slump
Replies: 6
Views: 11075

Did you make your drop ring? If you purchased it where did you get it?
Thanks, Stephie
by Stephie
Wed Dec 10, 2003 8:24 pm
Forum: Techniques and Tools
Topic: slumping overhang
Replies: 5
Views: 11216

Is it better to slump lower for longer to not pick up the texture?
Stephie
by Stephie
Fri Dec 05, 2003 5:26 pm
Forum: Techniques and Tools
Topic: Need help in how to fire a regular kiln for fusing and slump
Replies: 7
Views: 12661

Hi Sande, I also use a ceramic kiln. You can get a pyrometer (sp?) and probe (thermocouple) for less then $100. I drilled a hole in my peep hole plug to put the probe through. This lets me monitor the temp in the kiln and adjust the infinite switch accordingly. I think you are going to have to monit...
by Stephie
Thu Dec 04, 2003 6:15 pm
Forum: Techniques and Tools
Topic: Fire polish after slump?
Replies: 11
Views: 24278

Charlies right! I had a bowl that was great except I thought it should be a bit more shiney (is that a word?), any way, my bowl is now a needlely mess that distorted the pattern on the way down. I'll be making it's replacement this weekend. :roll:
It was a good learning experience!
by Stephie
Thu Dec 04, 2003 5:02 pm
Forum: Techniques and Tools
Topic: SS Rings
Replies: 7
Views: 12752

Does he have a web site?
Stephie
by Stephie
Thu Dec 04, 2003 11:42 am
Forum: Techniques and Tools
Topic: Pyrometers..plates...bubbles agrhhhh!
Replies: 16
Views: 28553

Here is another place to get thermo & pyrometers.
http://www.omega.com/
by Stephie
Wed Dec 03, 2003 12:19 pm
Forum: Techniques and Tools
Topic: I've got blisters on me fingers
Replies: 10
Views: 18387

How about good ole duck tape? :wink:
by Stephie
Mon Dec 01, 2003 2:39 pm
Forum: Business Topics
Topic: Glass Eye 2000
Replies: 4
Views: 8384

Karen,
Have you gone through the tutorials? They cover a great deal.
Stephie
by Stephie
Fri Nov 14, 2003 4:15 pm
Forum: Techniques and Tools
Topic: sinkhole question
Replies: 6
Views: 10958

Charlie, you've been hanging around with Brock haven't you? :P
by Stephie
Thu Nov 13, 2003 11:36 am
Forum: Techniques and Tools
Topic: Setting up a warm glass studio.....
Replies: 40
Views: 73612

:wink: That has to be a joke!
by Stephie
Wed Nov 12, 2003 1:16 pm
Forum: Techniques and Tools
Topic: Atten: Jewelry Pendant artist
Replies: 17
Views: 33353

Thanks for the tip Sadie!
by Stephie
Wed Nov 12, 2003 12:35 pm
Forum: Techniques and Tools
Topic: Atten: Jewelry Pendant artist
Replies: 17
Views: 33353

Sorry I can't help with a site, but the general term for these type of items is Findings. You may want to a seach for a findings wholesaler.