Search found 3 matches

by KissMyGlass
Tue Sep 11, 2012 1:02 am
Forum: Newcomer Forum
Topic: deep drop ceramic mold
Replies: 2
Views: 9166

deep drop ceramic mold

I have a very deep ceramic mask mold. I have fired this mask twice. The first time I didn't quite know what to look for when I peeked into the kiln, so I know I didn't leave it in long enough. I took it to 1175 for 30 min. I fired it a second time, took it to 1250 for two hours, it still hadn't fill...
by KissMyGlass
Tue Jun 26, 2012 9:47 am
Forum: Newcomer Forum
Topic: slumping
Replies: 1
Views: 7204

slumping

I have a mask that I slumped that didn't get completely finished. Can I put it back in and redo it and if so at what temperature.
Marla
by KissMyGlass
Sat Jun 16, 2012 9:12 am
Forum: Newcomer Forum
Topic: masks
Replies: 3
Views: 11130

masks

I have a new mask mold. I thought I'd use the spray instead of kiln wash due to the tiny places. It is a pretty deep mold. Do I cut the glass slightly larger that the edge of the mold? Anybody have any pointers?