Yea, just have to get after it, would prefer self scoring and snapped glass , but it wasn't under the tree this year
Wyndham
Search found 12 matches
- Fri Dec 26, 2014 2:00 pm
- Forum: Techniques and Tools
- Topic: Cutting glass with a dremel diamond disk
- Replies: 7
- Views: 11468
- Tue Dec 23, 2014 5:52 pm
- Forum: Techniques and Tools
- Topic: Cutting glass with a dremel diamond disk
- Replies: 7
- Views: 11468
Cutting glass with a dremel diamond disk
I've got some CBS dichroic thin glass1"x6" glass that I'm looking to find an efficient method of cutting with a saw. Several years ago I had a table top glass bandsaw but had many issues with the guides and the blade. I have recently gotten a dremel diamond wheel that seems to work well at...
- Mon Dec 03, 2012 1:11 pm
- Forum: Newcomer Forum
- Topic: kiln for slumping q?
- Replies: 2
- Views: 3927
kiln for slumping q?
I have seen where some glass fusing/slumping kilns are designed with elements in the lid of the kiln. My kiln has 3 zone type s thermocouples that I use in my pottery glaze firings. Is there an advantage to kilns for glass fusing/slumping or a major disadvantage in using a kiln with side and a botto...
- Mon Dec 03, 2012 1:00 pm
- Forum: Newcomer Forum
- Topic: kiln wash and bisque mold
- Replies: 2
- Views: 3997
Re: kiln wash and bisque mold
Thanks Brad. 80/20 sounds good
Wyndham
Wyndham
- Mon Dec 03, 2012 12:23 am
- Forum: Newcomer Forum
- Topic: kiln wash and bisque mold
- Replies: 2
- Views: 3997
kiln wash and bisque mold
Hi folks, I'm a potter that is looking to getting into slump glass.I plan to make some bisque flat rectangular trays. My kiln wash for my pottery is 1/3 alumina hydrate, 1/3 kaolin clay, 1/3 350 mesh silica. Should i leave out the silica and go 50/50 kaolin/alumina hydrate? I'm looking to fuse a bas...
- Tue Jul 22, 2003 12:07 pm
- Forum: Techniques and Tools
- Topic: channel for pendant?
- Replies: 3
- Views: 4266
thanks
Thanks for the info, will try with next batch. wyndham@ac.net
- Tue Jul 22, 2003 10:24 am
- Forum: Techniques and Tools
- Topic: channel for pendant?
- Replies: 3
- Views: 4266
channel for pendant?
I am trying to figure out a way to put a channel in a fused multi-layer pendant to hang on a chain. Should I use a nichrome wire coated with kiln wash , where the wire rest on a base piece of glass and the coated wire is sandwiched between or make up a coil of kiln wash the same dia, as the channel ...
- Thu Jul 03, 2003 1:47 pm
- Forum: Techniques and Tools
- Topic: glass thickness ?
- Replies: 13
- Views: 11222
thanks for the input
Well, this is kinda what I was thinking might be the case, gravity works. Thanks for the input. Would putting a weight on top of a piece be a problem when the glass cools at 960 quarts inversion? I'll try with a broken piece of kiln shelf and post later. Thanks wyndham@ac.net
- Thu Jul 03, 2003 10:08 am
- Forum: Techniques and Tools
- Topic: glass thickness ?
- Replies: 13
- Views: 11222
glass thickness ?
I am new to fusing and am learning much as each firing comes out. From what I have read on this board and other info, glass is going to go to 1/4 in thickness if fired to full fuse and over. my question is what temp over full fuse or what flux can be applied to the glass to allow it to flow back to ...
- Wed Jul 02, 2003 11:38 am
- Forum: Techniques and Tools
- Topic: Re: Pyrometer Creep
- Replies: 6
- Views: 7266
thermocouple drift
If your thermocouple is the thick twisted wire with ceramic spacers this is an older style and more prone to drift. There is a newer metal tude style that seems less prone to drift. Price should be 30-40 $ Type k They can drift in temp over time. As a way of calibrating your firing, get a box of pyr...
- Sat Jun 28, 2003 2:55 pm
- Forum: Techniques and Tools
- Topic: wasser glass fusing temp needed
- Replies: 2
- Views: 3491
wasser tech sheet
Thanks Brock , got the info
- Sat Jun 28, 2003 2:03 pm
- Forum: Techniques and Tools
- Topic: wasser glass fusing temp needed
- Replies: 2
- Views: 3491
wasser glass fusing temp needed
I am new to glass fusing. My wife and I are getting into fused jewelry with dichroic glass. We have come upon a supply of thin wasser glass already cut to shape and fired to a clean rounded edge . I need to know if a piece (1''x1") that has been fired, does that change the fusing temp if this g...