Search found 2 matches

by Glenburn
Mon Jun 30, 2003 11:23 am
Forum: Kiln Casting
Topic: Help needed with "Milk Glass"
Replies: 3
Views: 8920

Bert, Thanks for replying to my question on "milk glass". Your answer sounds intriguing and right up my alley. I am definately going to try using those glass beads once I find them. Thanks for the tip on a slump test as well. This was my first time on the bulletin board and I'm delighted t...
by Glenburn
Sun Jun 29, 2003 3:53 pm
Forum: Kiln Casting
Topic: Help needed with "Milk Glass"
Replies: 3
Views: 8920

Help needed with "Milk Glass"

I am interested in casting with "Milk Glass". I don't know if it is available to purchase anywhere. It is important to the project that an opaque white color glass is used and even better if it is considered milk glass. If anyone has any knowledge or information, I would appreciate it. Tha...