nope. treat it just like it is a product called "ZYP".
paint it on, let it dry for about 30 min. and you are good to go.
The Other Jim
Search found 454 matches
- Mon Nov 02, 2020 6:43 pm
- Forum: Newcomer Forum
- Topic: Boron Nitride POWDER
- Replies: 4
- Views: 26464
- Sun Nov 01, 2020 11:50 am
- Forum: Newcomer Forum
- Topic: Boron Nitride POWDER
- Replies: 4
- Views: 26464
Re: Boron Nitride POWDER
Mix the powder with water to a cream consistency and paint it on like you would kiln wash.
I have used it on SS and clay fired stuff with good results.
The other Jim
I have used it on SS and clay fired stuff with good results.
The other Jim
- Tue Oct 27, 2020 1:44 pm
- Forum: Newcomer Forum
- Topic: Drop with Dropring
- Replies: 16
- Views: 49625
Re: Drop with Dropring
No, Jan you didn't do anything wrong. That link was supposed to show you how to do a drop with only one firing. That post and the firing schedule were first posted by me, and I do not seem to find it either. I will look and see if I can find a link that works, and if I can. I will post it here. The ...
- Wed Sep 30, 2020 12:25 pm
- Forum: Newcomer Forum
- Topic: bubbles
- Replies: 2
- Views: 24642
Re: bubbles
I am sorry to inform you that if these are "micro"bubbles, then you are stuck with them unless you can figure
out a way to remelt the glass and hold for a long time.
The other Jim
out a way to remelt the glass and hold for a long time.
The other Jim
- Sat Sep 05, 2020 12:26 pm
- Forum: Techniques and Tools
- Topic: How to Fire Dichroic and Retain Colour
- Replies: 7
- Views: 9828
Re: How to Fire Dichroic and Retain Colour
What Kevin said, Also the color will shift across the same sheet.
The other Jim
The other Jim
- Sat Aug 29, 2020 12:24 pm
- Forum: Newcomer Forum
- Topic: frit lace rescue
- Replies: 5
- Views: 17265
Re: frit lace rescue
Hey, Michael.
Would you be so kind as to let us know how your 2nd firing on the kiln paper turned out?
Thanks.
The other Jim
Would you be so kind as to let us know how your 2nd firing on the kiln paper turned out?
Thanks.
The other Jim
- Mon Aug 24, 2020 12:23 pm
- Forum: Newcomer Forum
- Topic: frit lace rescue
- Replies: 5
- Views: 17265
Re: frit lace rescue
as long as the paper is not torn or disturbed and you can not see the kiln shelf, you can reuse it.
The other Jim
The other Jim
- Sat Aug 15, 2020 6:18 pm
- Forum: Newcomer Forum
- Topic: Freeze and Fuse firing cycle
- Replies: 16
- Views: 38154
Re: Freeze and Fuse firing cycle
I also use an old electric tooth brush held onto the side of the mold.
This vibrates the powder and gets all of the excess water out.
The other Jim
This vibrates the powder and gets all of the excess water out.
The other Jim
- Thu Aug 13, 2020 7:22 pm
- Forum: Business Topics
- Topic: Glass/Cash Survey
- Replies: 12
- Views: 65092
Re: Glass/Cash Survey
Sometimes you are NOT charging enough. When I was doing shows, I ran into a situation than I was charging $4.00 for some coasters. One of the vendors told me to raise the price. I asked her "why" they are not selling now. Well I tried and raised the price to $9.00 and sold every one. Who k...
- Sat Aug 08, 2020 1:07 pm
- Forum: Techniques and Tools
- Topic: Cracked during heat up
- Replies: 15
- Views: 15922
Re: Cracked during heat up
It does look to me that it is an incompatibly problem. Maybe some of the glass shifted in the combing cycle. I have had that happen to me before. There is a lot more than COE involved in the heating process. I suggest that you stick to the same manufacturer. I also suggest that you read the BE artic...
- Thu Jul 23, 2020 11:39 am
- Forum: Techniques and Tools
- Topic: bottom heat kiln.
- Replies: 11
- Views: 16484
Re: bottom heat kiln.
As long as you are having it built, why don't you have a switch installed so you can turn the bottom elements off?
The other Jim
The other Jim
- Fri Jul 17, 2020 12:23 pm
- Forum: Techniques and Tools
- Topic: melted mess
- Replies: 4
- Views: 5724
Re: melted mess
Should e just fine, I did exactly what Brad did about 6 years ago and it is working just fine.
The other Jim
The other Jim
- Thu Jul 09, 2020 12:09 pm
- Forum: Newcomer Forum
- Topic: Paragon Infinite Control Switch
- Replies: 1
- Views: 8135
Re: Paragon Infinite Control Switch
Set them all on high and leave them there.
The other Jim
The other Jim
- Sat Jul 04, 2020 11:43 am
- Forum: Techniques and Tools
- Topic: FIRE POLISHING
- Replies: 11
- Views: 13518
Re: FIRE POLISHING
Myself, I would go to an 800 grit before fire polish.
If you have the means, then go all of the way through cerium oxide.
This will give you a surface that is equal to float glass.
The other Jim
If you have the means, then go all of the way through cerium oxide.
This will give you a surface that is equal to float glass.
The other Jim
- Mon Mar 16, 2020 12:03 pm
- Forum: Techniques and Tools
- Topic: FUSING HOUSE NUMBERS
- Replies: 3
- Views: 6002
Re: FUSING HOUSE NUMBERS
What Don said. ABSOLUTELY
The other Jim
The other Jim
- Sun Feb 23, 2020 2:52 pm
- Forum: Techniques and Tools
- Topic: Fiber Kiln/Shelf
- Replies: 11
- Views: 38484
Re: Fiber Kiln/Shelf
Bullseye sells ABSOLUTELY the flattest kiln shelf out there. Shipping cost might be a problem, but I think in the long run it would be worth it. Shelves from a ceramic supply store may or may not be absolutely flat. A flat shelf is really necessary for a lot of different kinds of firings. Just my $0...
- Sun Feb 16, 2020 2:12 pm
- Forum: Photos and Stuff
- Topic: cut, carved and polished
- Replies: 5
- Views: 28488
Re: cut, carved and polished
Love it.
the other Jim
the other Jim
- Tue Nov 19, 2019 1:40 pm
- Forum: Techniques and Tools
- Topic: Silver foil & leaf
- Replies: 9
- Views: 10542
Re: Silver foil & leaf
Thanks for posting the results. That is one of the reasons that this board is so darned good.
People like you that have a question that needs answered and then discover a cure on their own, then publish the results for the rest of us.
Thank you so much.
The other Jim
People like you that have a question that needs answered and then discover a cure on their own, then publish the results for the rest of us.
Thank you so much.
The other Jim
- Tue Nov 12, 2019 11:51 am
- Forum: Techniques and Tools
- Topic: Silver foil & leaf
- Replies: 9
- Views: 10542
Re: Silver foil & leaf
There is a product called "Tarnex" that works wonders.
Just dip the silver in and the tarnish comes off in about 1 or 2 seconds at the most.
Ten just immerse in hot water , pull out, let dry and you are good to go.
The other Jim
Just dip the silver in and the tarnish comes off in about 1 or 2 seconds at the most.
Ten just immerse in hot water , pull out, let dry and you are good to go.
The other Jim
- Wed Sep 04, 2019 3:34 pm
- Forum: Newcomer Forum
- Topic: ridigizer with fiberboard
- Replies: 4
- Views: 14865
Re: ridigizer with fiberboard
OK, thanks Kevin
I will try the fiberboard.
Will I need to apply a glass separator?
The other Jim.
I will try the fiberboard.
Will I need to apply a glass separator?
The other Jim.