Search found 1 match

by Rich Canby
Thu Jan 24, 2013 5:22 pm
Forum: Newcomer Forum
Topic: Adding glass during a slump ?
Replies: 20
Views: 54435

Re: Adding glass during a slump ?

Wondering if you had any success? I am doing similar stuff. Successfully fuzed multiple layers of glass to make a 24" circle 1 1/4" thick. I have been rough grinding it for a couple of weeks. Sagitta is at .090" but I need about .28". This is how deep the central depression is. I...