Search found 14 matches
- Mon Dec 16, 2013 3:40 pm
- Forum: Techniques and Tools
- Topic: Pattern Bars help
- Replies: 1
- Views: 3604
Pattern Bars help
Hi, We are doing some pattern bars. We have slices about 1"x2" (sort of domino size). If we want to have them all in a row down the center of a platter, do you recommend us to first fuse the sliced pieces into a solid piece and then add the rest of the platter glass around it, or do you te...
- Mon Dec 16, 2013 3:37 pm
- Forum: Techniques and Tools
- Topic: Belt Sander or Lap Wheel
- Replies: 6
- Views: 8096
Belt Sander or Lap Wheel
Hi, we have a small fused glass business and want to keep expanding our tools for the studio. I was curious, of your thoughts on tools. We have a wet saw and grinder, and ringsaw, but are thinking about getting either a lapwheel sander or a sanding belt sander to do more of the coldworking/finishing...
- Fri May 10, 2013 8:46 am
- Forum: Business Topics
- Topic: Small Business - insurance
- Replies: 4
- Views: 7500
Small Business - insurance
Hi, I was just curious, for any of you that have a small business selling your glass items, do you carry any special insurance for that? I wasn't sure if you ever felt you had to have something in place in case someone was injured on your piece somehow.
Thanks
Cherie
Thanks
Cherie
- Fri May 03, 2013 8:12 pm
- Forum: Techniques and Tools
- Topic: Fusing little dots
- Replies: 13
- Views: 18600
Re: Fusing little dots
Thanks everyone for the quick replies. We will work to change our length. We had a full shelf with about 30 of these dots all different colors. Our firing schedule had been: Segment Rate Temp Soak (Hold) 1 500 1495 .15 2 AFAP 900 2.00 3 AFAP 100 2.00 Thanks. Cherie
- Fri May 03, 2013 3:47 pm
- Forum: Techniques and Tools
- Topic: Fusing little dots
- Replies: 13
- Views: 18600
Fusing little dots
Hi, We were trying to make a lot of dots to then apply to some plates. We noticed when we do full fuse of a 3/4"x3/4" square black glass (stacked 3 high) it fuses into a nice round circle. But we noticed if we do identical setup for White or red it seems like they all get jagged edges arou...
- Thu May 02, 2013 12:50 pm
- Forum: Techniques and Tools
- Topic: Shelf Primer dust
- Replies: 10
- Views: 11498
Re: Shelf Primer dust
We were wondering if we shouldn't just scrub off and reapply Bullseye shelf primer before each fusing. It just gets to be a lot of work to do it every time though but if we keep having all these pieces show up all powdered and unable to get a clean bottom we probably need to do that. Just curious fo...
- Tue Apr 30, 2013 7:19 pm
- Forum: Techniques and Tools
- Topic: Cabinets to hold glass
- Replies: 3
- Views: 4649
Cabinets to hold glass
Hi, does anyone know of any business that might sell cabinetry that we could use to store our glass. We basically have a lot of 1/2 sheets and then 1/4 sheets of glass and we want to put in a cabinet in our studio to house all of this glass. We thought about making it ourselves, but I wondered if an...
- Mon Apr 29, 2013 11:59 pm
- Forum: Techniques and Tools
- Topic: Shelf Primer dust
- Replies: 10
- Views: 11498
Re: Shelf Primer dust
So you recommend just a mist across the shelf, do I then rub it down at all or just let it set?
- Mon Apr 29, 2013 9:54 am
- Forum: Techniques and Tools
- Topic: Attaching findings to pendants
- Replies: 6
- Views: 7753
Re: Attaching findings to pendants
I had tried a little tube of the E6000 but it just seems so stringy I had a harder time applying without getting glue all over everything. Maybe just user error
- Sun Apr 28, 2013 10:46 pm
- Forum: Techniques and Tools
- Topic: Gryphon Ring Saw accessories?
- Replies: 1
- Views: 3165
Gryphon Ring Saw accessories?
Hi, we have not been able to locate accessories for the Gryphon ring saw we recently bought. I really wish we had a straight edge to attach so that it would make using the blade for straight cuts much easier? We noticed some of the Taurus 3 items almost look like they would work with Gryphon as well...
- Sun Apr 28, 2013 10:25 pm
- Forum: Techniques and Tools
- Topic: Attaching findings to pendants
- Replies: 6
- Views: 7753
Attaching findings to pendants
Hi, what does everyone recommend as a good adhesive to attach findings?
Thanks
Cherie
Thanks
Cherie
- Sun Apr 28, 2013 10:24 pm
- Forum: Techniques and Tools
- Topic: Shelf Primer dust
- Replies: 10
- Views: 11498
Shelf Primer dust
We use Bullseye Shelf Primer on our kiln shelves and fuse all of our pieces on the shelf directly. We've let it go several times before we re-apply the wash. It always seems to have a really fine powder on the shelf all the time. Do you all clean /vacume shelves after each use? We notice sometimes w...
- Tue Apr 23, 2013 11:59 pm
- Forum: Business Topics
- Topic: Glass Studio Setup
- Replies: 2
- Views: 7443
Glass Studio Setup
Hi, We are setting up our home studio and wondering if anyone has posted pictures of different examples of their own studios? In particular,what sort of cabinets or storage do people like to use to store all their different glass? We are looking at getting a cabinet made and looking for pictures of ...
- Tue Apr 23, 2013 11:32 pm
- Forum: Techniques and Tools
- Topic: Oval dish suggestions
- Replies: 3
- Views: 4338
Oval dish suggestions
Hi, We bought an oval mold from Bullseye and I was wondering about the typical process folks use. Do you make your initial item cut to the shape of the oval first, or do you instead make the item originally in an oblong sort of size and then once fully fused cut it with a saw to shape to the size of...