Search found 4 matches

by Mack Davis
Tue May 28, 2013 10:39 pm
Forum: Techniques and Tools
Topic: Glass separation
Replies: 14
Views: 24331

Re: Glass separation

for the green and black: 300 To 900 hold 15, 100 to 1200 H 40, Full to 1450 h 30, 1000 to 960 h60, 200 to 725 h 10, 400 to 100 h 0, original firing, the clear piece was originally fused with this for the clear piece it was the same except high temp was 1475, there were other pieces in both firings t...
by Mack Davis
Tue May 28, 2013 9:06 pm
Forum: Techniques and Tools
Topic: Glass separation
Replies: 14
Views: 24331

Re: Glass separation

Pictures
by Mack Davis
Tue May 28, 2013 8:57 pm
Forum: Techniques and Tools
Topic: Glass separation
Replies: 14
Views: 24331

Re: Glass separation

The glass is 96 coe, there were two different firings. There were other pieces in both that fused correctly. Two were almost exactly the same, one piece was perfect, the other split and then moved.
by Mack Davis
Mon May 27, 2013 10:51 pm
Forum: Techniques and Tools
Topic: Glass separation
Replies: 14
Views: 24331

Glass separation

What causes glass separating and moving in the kiln. The pieces were fully fused