I thought it might be interesting for some to see the process in creating the color bars since we lost a bunch of older posts on how to create. Hope it might help a few artists to create with movement and fun.
Search found 560 matches
- Thu Aug 02, 2012 2:42 pm
- Forum: Photos and Stuff
- Topic: Uroboros Residency
- Replies: 44
- Views: 42445
- Mon Jul 30, 2012 7:48 pm
- Forum: Photos and Stuff
- Topic: Uroboros Residency
- Replies: 44
- Views: 42445
Re: Uroboros Residency
Hi Havi, have not talked to you for some time now. Have been away in the U.S.A. creating and enjoying Uroboros Glass Company so much. The last one is a corner of the middle Cast Piece . It is the 27 inch by 27 inch by 1 inch. I had alot of fun creating the color bars and then re-investing into the c...
- Fri Jul 27, 2012 12:04 pm
- Forum: Photos and Stuff
- Topic: What to do with vitrigraph stuff
- Replies: 40
- Views: 81358
Re: What to do with vitrigraph stuff
Amazing work both of you. Love the cane work for sure.
Leslie
Leslie
- Thu Jul 26, 2012 5:09 pm
- Forum: Photos and Stuff
- Topic: Uroboros Residency
- Replies: 44
- Views: 42445
Re: Uroboros Residency
Thankyou so very much fellow Calgary Glass Guild member and always helper. Soon I hope to have a new computer. First I have to STOP purchasing glass.
Les
Les
- Thu Jul 26, 2012 12:48 pm
- Forum: Photos and Stuff
- Topic: Uroboros Residency
- Replies: 44
- Views: 42445
Re: Uroboros Residency
http://www.bullseyeglass.com/index.php?option=com_jfusion&Itemid=224&jfile=viewtopic.php&f=14&t=161 I know we lost alot of our early posts here on warmglass so for some that did not see alot of all our discussions and sharing, this one comes to mind in helping to show how creative we...
- Wed Jul 25, 2012 11:20 pm
- Forum: Photos and Stuff
- Topic: Uroboros Residency
- Replies: 44
- Views: 42445
Re: Uroboros Residency
Thanks so much Shawn, I wish I lived closer to Victoria , B.C. and we could go for a walk on the boardwalk as I miss the ocean so very much. I hear you are visiting there. Perhaps a few other artists on the island could send you a private PM and hook up with you. When I get some nice professional pi...
- Wed Jul 25, 2012 3:04 pm
- Forum: Photos and Stuff
- Topic: Uroboros Residency
- Replies: 44
- Views: 42445
Re: Uroboros Residency
This is the larger one but the back side of it. It is 46 inch x 22 inch x 1 inch
- Wed Jul 25, 2012 2:58 pm
- Forum: Photos and Stuff
- Topic: Uroboros Residency
- Replies: 44
- Views: 42445
Uroboros Residency
phpoPpBT4AM.jpg I thought I would share what I was up to at my Uroboros Residency in Portland. It was truly wonderful and met some wonderful artists , and of course the owners and Kat and Bill and all the staff are totally super. Carol Carson and I finally met and we laughed so hard because we both...
- Sat Jul 21, 2012 1:09 pm
- Forum: Photos and Stuff
- Topic: Finally some new images from my Tropical Woman series
- Replies: 27
- Views: 35646
Re: Finally some new images from my Tropical Woman series
Raphael, as always, it is truly stunning work. You have captured such wonderful personality . I love the hair in both pieces and thankyou so very very much for sharing the progression shots. I hope you love firing on my Dyson shelves too that you so kindly helped me store at your studio , and was so...
- Sat Dec 29, 2007 8:35 pm
- Forum: Kiln Casting
- Topic: Zircon shell moulds
- Replies: 0
- Views: 9016
Re: Zircon shell moulds
http://i228.photobucket.com/albums/ee40/twin_vision_glass/SMALLT2.jpg Hello, Well to start off with it is an honour to be discussing mold materials with you Colin. I have watched your work for many years. My twin and I have been using Zircar Mold Mix 6 for many years and this is a picture of a piec...
- Sun Dec 16, 2007 1:47 pm
- Forum: Kiln Casting
- Topic: Bear Facts
- Replies: 14
- Views: 25524
Re: Bear Facts
Just a very light dusting of spray though so you don't change the texture of the piece. Les
- Sat Dec 15, 2007 1:51 pm
- Forum: Photos and Stuff
- Topic: New Panels
- Replies: 6
- Views: 10221
Re: New Panels
Not at all Haydo!!! This has always been my major problem.I am the first to admit it. I live so far away from the city and to get a stand (or even new clips soldered onto the tall stand you see here) (which is not finished yet ) and I tried to say this in the beginning of the thread but sorry I was ...
- Sat Dec 15, 2007 2:15 am
- Forum: Photos and Stuff
- Topic: New Panels
- Replies: 6
- Views: 10221
Re: New Panels
Well thanks to all who enjoy our beautiful surroundings as much as I do. In all parts of the world there is unique environmental inspiration. We cannot help but be influenced by the spectacular mountains, rivers and lakes, just as you are influenced by flowers and pieces you carve Peter. . Les
- Fri Dec 14, 2007 2:18 pm
- Forum: Kiln Casting
- Topic: Bear Facts
- Replies: 14
- Views: 25524
Re: Bear Facts
Dear Tom, there are sooo many great products out there . I am so glad that you are experimenting and loving the results. The nice thing about rubber is that it will last for many many years and is plyable so that undercuts are not a problem and it peels off like a glove. Would love to see some of yo...
- Fri Dec 14, 2007 12:50 pm
- Forum: Kiln Casting
- Topic: Bear Facts
- Replies: 14
- Views: 25524
Re: Bear Facts
Oh Ellen, isn't that funny. My family walks by doing this #-o as the piece gets larger and larger. I try to make things tiny, but well, if it is small it usually sits infront of something larger. I feel as if we are the luckiest people on earth to be able to create. I truly love the creation almost ...
- Fri Dec 14, 2007 2:18 am
- Forum: Photos and Stuff
- Topic: New Panels
- Replies: 6
- Views: 10221
Re: New Panels
Dear Sheila and Barb, thankyou for those kind words. I would love to pursue a Gallery in the U.S. again and am going to pound the pavement I think and look for one in the Portland area as it gives me a great reason to travel there .I love Portland. Now that my twin and I have stepped back from teach...
- Fri Dec 14, 2007 2:04 am
- Forum: Kiln Casting
- Topic: Bear Facts
- Replies: 14
- Views: 25524
Re: Bear Facts
Lynne, here is the last one that hopefully shows how thick it is and the overhang for strength at the edge . Les
- Fri Dec 14, 2007 2:02 am
- Forum: Kiln Casting
- Topic: Bear Facts
- Replies: 14
- Views: 25524
Re: Bear Facts
http://i228.photobucket.com/albums/ee40/twin_vision_glass/P1010649.jpg I hope this has helped . The last one is the rubber cut so that it comes off well. It is also important as you are painting on the rubber to make sure that you thicken where you are going to cut the rubber so the seem is not fli...
- Fri Dec 14, 2007 1:58 am
- Forum: Kiln Casting
- Topic: Bear Facts
- Replies: 14
- Views: 25524
Re: Bear Facts
http://i228.photobucket.com/albums/ee40/twin_vision_glass/P1010650.jpg Lynne, here is the mother mold laid out after coming off in special pieces made specifically where no undercuts are , this is why all the 5 parts or whatever it takes. I will post 2 more pics so you can see it being build piece ...
- Fri Dec 14, 2007 1:24 am
- Forum: Kiln Casting
- Topic: Bear Facts
- Replies: 14
- Views: 25524
Re: Bear Facts
Hi Lynne, where to start with the questions. let's start with no wax bits. I scrape with my scrapers and scope it up, roll it up in my fingers and press it back onto the piece to make hair or change the nose or something. I use a wheller gun to weld bits and pieces onto or off of him as I go. It is ...