razor blade.
there's also a chemical that can dissolve it. i believe home depot carries it.
Search found 958 matches
- Wed May 20, 2015 11:43 pm
- Forum: Newcomer Forum
- Topic: Removing unwanted GE Silicone II
- Replies: 6
- Views: 11702
- Sat May 16, 2015 10:08 am
- Forum: Techniques and Tools
- Topic: Anyone know where to buy this?
- Replies: 6
- Views: 9771
Re: Anyone know where to buy this?
find a local welder. they're probably pretty easy to make.
- Sun Apr 19, 2015 2:35 pm
- Forum: Techniques and Tools
- Topic: Cold combing
- Replies: 2
- Views: 5033
Re: Cold combing
if you get over 212F, you'll get steam and possibly movement. you might test out 160-180 and see how long it would take to dry. you can hold a mirror at one of the peepholes and see if you get any condensation. if not, it's probably dry.
- Wed Feb 25, 2015 12:05 am
- Forum: Newcomer Forum
- Topic: graphite
- Replies: 4
- Views: 9480
Re: graphite
you buy them. it depends upon how big you need. marble or bead makers use them. you can probably get them off ebay cheaply.
- Wed Feb 25, 2015 12:02 am
- Forum: Techniques and Tools
- Topic: Cutting circle from mullite kiln shelf
- Replies: 12
- Views: 24675
Re: Cutting circle from mullite kiln shelf
i would take a diamond blade in a 4" side angle grinder, and carefully lower the blade into the discarded piece near where the edges of the hole will be. make many cuts, and use the edge of it to round off and smooth (and probably bevel) the hole sides. make shallow cuts, deepening them with mu...
- Sat Feb 14, 2015 1:31 pm
- Forum: Business Topics
- Topic: Designing a new studio
- Replies: 38
- Views: 61904
Re: Designing a new studio
[quote="Mark Hall"]Don't forget good ventilation, especially working with powders. I prefer a whole house fan mounted at the end of the bench, blowing out. Somewhere you can brush off your work that's filled with stuck fiber paper & such. A portable fan can be positioned to create hori...
- Sat Feb 14, 2015 1:28 pm
- Forum: Techniques and Tools
- Topic: GE Silicone II
- Replies: 11
- Views: 19454
Re: GE Silicone II
i like the ace hardware crystal clear silicone over ge. it cures a lot clearer. ge seems to get milky as it cures. it is a bit more than ge though. i never seem to finish a large tube, so the smaller ones, although more expensive per oz, is actually cheaper because i don't have to throw away as much...
- Fri Feb 06, 2015 12:28 am
- Forum: Techniques and Tools
- Topic: source for float glass
- Replies: 6
- Views: 9763
Re: source for float glass
yard sales. think chipped dining room or living room tabletops. i've gotten pieces up to 1.5" thick for a few dollars.
- Sat Jan 31, 2015 3:56 pm
- Forum: Techniques and Tools
- Topic: 2mm Clear 96
- Replies: 5
- Views: 6508
Re: 2mm Clear 96
the hotter you go, the more it will shrink because it's trying to get to 6mm overall. you might get dogboning or something similar.
- Sat Jan 17, 2015 12:08 am
- Forum: Techniques and Tools
- Topic: Hang your Glass glue
- Replies: 16
- Views: 28984
Re: Hang your Glass glue
i made a couple of stacks of float glass, glued with UV water thin glue i got at home depot as feet for a sheet of glass over an LED lightbulb. the glue was water clear and disappeared. about 7 years now. i also made some stacks of float glass to glue on sheets of glass I use on top of my salt water...
- Fri Jan 16, 2015 11:58 pm
- Forum: Kiln Casting
- Topic: Removing Plaster from Mold
- Replies: 16
- Views: 27625
Re: Removing Plaster from Mold
take it to the car wash and use their washer. it's not as powerful as a purchased power washer, because no one likes removing the paint from their car.
- Fri Jan 09, 2015 3:12 am
- Forum: Techniques and Tools
- Topic: Sandblasting Question
- Replies: 7
- Views: 8346
Re: Sandblasting Question
it's fusing. you can't get all sides to be shiny. whatever is against a mold will always be matte to some degree. a blasted surface will be even more matte than a non-blasted surface, if it's against a shelf.
- Wed Jan 07, 2015 12:16 am
- Forum: Techniques and Tools
- Topic: Fire Polish 2.0 / Matte Finish
- Replies: 4
- Views: 6002
Re: Fire Polish 2.0 / Matte Finish
i do a matte at 1225 for 7 minutes. leave it in the mold, or you risk it unslumping.
- Wed Jan 07, 2015 12:15 am
- Forum: Techniques and Tools
- Topic: French Cleats or Hanging glass panels
- Replies: 4
- Views: 7925
Re: French Cleats or Hanging glass panels
anyone with a table saw can make french cleats. try a home handyman, or a shop that makes kitchen cabinets. it's basically a piece of wood or plexiglass, maybe around 10cmx20cmx8mm, cut in half the long way on a 45 degree angle. screw one side to the wall, glue the other side (i use silicone) to the...
- Mon Jan 05, 2015 11:46 pm
- Forum: Techniques and Tools
- Topic: Fire Polishing
- Replies: 4
- Views: 5917
Re: Fire Polishing
i'm not sure 5 min at 1275 will firepolish. it won't in my kiln. i'd get a light matte surface.
you should look in at 1275, and see if it's shiny enough for you. if not, just increase the time.
you should look in at 1275, and see if it's shiny enough for you. if not, just increase the time.
- Sun Jan 04, 2015 5:24 pm
- Forum: Newcomer Forum
- Topic: Slumping disaster - HELP!
- Replies: 4
- Views: 7112
Re: Slumping disaster - HELP!
as the heat has undoubtably caused the glass to stretch, when you flatten it, it won't be round or even again, but distorted.
you can either start over, or use a large flat lap to grind down the edge to make it even. you'd have to do this to all the bowls to make them match.
you can either start over, or use a large flat lap to grind down the edge to make it even. you'd have to do this to all the bowls to make them match.
- Sun Jan 04, 2015 5:22 pm
- Forum: Techniques and Tools
- Topic: Making a mold of a bowl
- Replies: 18
- Views: 26018
Re: Making a mold of a bowl
[quote="The Hobbyist"]I would make a plaster cast of the center medallion. Then roll out a flat circle of clay. Press the medallion into the center and hand carve the petals and scallop the edges. Check for any under cuts that need easing and then bisque the clay when it's dry. This will y...
- Sun Dec 07, 2014 11:29 pm
- Forum: Techniques and Tools
- Topic: BE ball mold?
- Replies: 18
- Views: 22799
Re: BE ball mold?
[quote="Vonon"]Charlie, Are the stands from Picazzo's for tableware - like for holding pizza or bread basket?[/quote] they are pizza stands for the table. they must get then from some supplier, because all the stores in the chain have the same ones, but no mgr that i've asked has been able...
- Sun Dec 07, 2014 6:42 pm
- Forum: Techniques and Tools
- Topic: BE ball mold?
- Replies: 18
- Views: 22799
Re: BE ball mold?
[quote="Babette (Shawn)"]I made a coiled steel stand for those totally round bottoms. Expensive and a bit excentric...[/quote] the stands at a place called Picazzo's (here in AZ) are perfect for this. i've bought stands from them for not very much. they look almost like this, except they'r...
- Fri Dec 05, 2014 10:58 pm
- Forum: Techniques and Tools
- Topic: Using spectrum cullet for pate de verre
- Replies: 21
- Views: 26989
Re: Using spectrum cullet for pate de verre
and put the magnet in a plastic bag first.